C85S, 1.1269, XC85, AISI 1086 - Low-alloy spring steel for oil hardening for lightweight springs according to EN 10132-4.

 

Standards Steel Grades
Chemical Composition %
C: Mn: Si: P: S: Cr: Mo: Ni: Cu:
EN C85S - 1.1269 - C 85 S - Ck85
0.80 - 0.90 0.40 - 0.70 0.15 - 0.35 <0.025 <0.025 <0.40 <0.10 <0.40 -
EN 2CS85
0.80 - 0.90 0.45 - 0.65 0.15 - 0.40 <0.035 <0.035 - - - -
AFNOR XC85 - XC 85
0.80 - 0.98 0.40 - 0.70 0.20 - 0.40 <0.04 <0.04 - - - -
ISO CS85 - CS 85
0.80 - 0.94 0.70 - 1.00 0.10 - 0.35 <0.035 <0.03 - - - -
BS CS80 - CS 80
0.75 - 0.85 0.50 - 0.90 0.05 - 0.35 <0.045 <0.045 - - - -
DIN CK 85 - Ck85
0.80 - 0.90 0.45 - 0.65 0.15 - 0.35 <0.035 <0.035 - - - -
DIN 85Cr1 - 85 Cr 1 - 1.2004 - 2004
0.80 - 0.90 0.50 - 0.70 0.30 - 0.50 <0.035 <0.035 0.30 - 0.45 - - -
PN gat. 85
0.82 - 0.90 0.50 - 0.80 0.17 - 0.37 <0.040 <0.040 <0.30 - <0.30 <0.25
DIN C85E - C 85 E
0.80 - 0.90 0.40 - 0.70 0.15 - 0.35 <0.025 <0.025 <0.40 <0.10 <0.40 -
GOST 85
0.82 - 0.90 0.30 - 0.70 0.17 - 0.37 <0.035 <0.035 <0.15 - <0.15 <0.20
ČSN
STN
ČSN 12 090 - 12090
0.80 - 0.90 0.20 - 0.60 <0.35 <0.030 <0.035 - - - -
AISI AISI 1086
0.80 - 0.93 0.30 - 0.50 - <0.04 <0.05 - - - -

 


C85S, 1.1269, AISI 1086 - specification and application

Non-alloyed carbon structural steel with low hardening capacity for oil hardening for low-duty, periodically operating springs, springs and spring elements, immune to the temper brittleness. It is characterized by its high hardness and abrasion resistance, while maintaining high strength. It is used for flat and spiral springs, machine parts or saws of all kinds for cutting.

Grade 85 and C85S steel are mainly used as steel for ball mills, press plates, stone saws, wire for steel ropes, briquetting press parts. C85S and 85 steels are non-weldable and resistant to corrosive environments due to their high carbon content and low levels of alloying additives. During heat treatment steel is vulnerable to decarburization and oxidation.


Mechanical properties of steel

Mechanical and physical properties
Heat-treated state C85S +QT
Tensile Strenght Rm 1200 - 2000 MPa
Hardness HRC HV 38.5 - 55.0 HRC 370 - 600 HV
Soft state after smoothing rolling C85S +A+LC
Tensile strenght Rm < 670 MPa
Yield point Re < 535 MPa
Elongation A > 15%
Hardness HRB HV < 94 HRB < 210 HV
Cold-rolled state C85S +CR
Tensile Strenght Rm < 1190 MPa
Hardness HV < 325 HV

 


Heat treatment process

Heat treatment
Process cooling Temperatures
Normalizing annealing w powietrzu 780 - 810℃
Softening annealing 660 - 700℃
Hardening in oil 810 - 830℃
Tempering in air 460 - 500℃

 


In the C85S, 1.1269 grades the company provides:

 


List of equivalents and other determinations of C85S steel:

C85S, 1.1269, C 85 S, Ck85, 2CS85, XC85, XC 85, CS85, CS 85, CS80, CS 80, CK 85, Ck85, gat. 85, C85E, C 85 E, 85, ČSN 12 090, ČSN 12090, AISI 1086, 85Cr1, 85 Cr 1, 1.2004, 2004


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.