Quality sheets and plates made of alloyed, special and stainless steels

 

 

 

Sheets and plates for Quenching and tempering, nitriding
16MnCr5 - 1.7131 20MnCr5 - 1.7147
30HGSA 15CDV6
25CrMo4 - 1.7218 - A829/A505/A506 Gr. 4130 42CrMo4 - 1.7225 - A829/A505/A506 Gr. 4140
C15 - 1.0401 - C15E - 1.1141 C22E - 1.1151 - st20
C60 - 1.0601 - C60E - 1.1221 C60W - 1.1740

 

 

Abrasive wear resistant sheets, plates
X120Mn12 - 1.3401 - 11G12 - Z120M12

 

 

We divide the sheets into thin and thick sheets. The offer of the VIRGAMET company includes Sheet Metal:

  • Sheets and plates made of thermal improvement steel
  • Spring, carbon and alloy plates
  • Carburizing plates
  • High-manganese wear-resistant steel sheets (Hadfield steel)
  • Chromium heat-resistant sheets, chromium-nickel sheets with aluminum, silicon, molybdenum, titanium additives etc.
  • Heat and creep resistant steel sheets
  • Stainless, acid-resistant, corrosion-resistant quarto sheets
  • Alloy sheets for heat-chemical treatment
  • Corrugated Corten sheets resistant to atmospheric corrosion
  • Manganese spring sheets 65G
  • Chromium-molybdenum sheets
  • Steel sheets of duplex type. superduplex
  • Chromium-manganese-silicon sheets
  • Ferrite and martensitic chromium sheets
  • Nitriding sheets
  • Tool steel sheets for hot and cold working
  • Tool sheets for shallow and deep quenching
  • Steel sheets of high-speed steel
  • Titanium and titanium alloys sheets
  • Nickel plates for low temperature operation
  • Boiler sheets for operation at higher temperatures and for pressure equipment
  • Bearing steel sheets
  • Superalloys sheets - nickel, chromium-nickel
  • Sheets of pure ARMCO iron
  • Hydrogen-resistant sheets at high pressures
  • Rolled sheets

Cold-rolled sheets made from stainless steel, duplex, heat-resistant steel, quenching and temperting steel, and spring steel

  • Cold rolled carbon structural alloyed steel sheets 0.5 to 4.0mm thick.
    • Formats: width 600 - 1500mm, length 2000 - 6000mm
  • Cold-rolled corrosion-resistant, acid-resistant, heat-resistant and stainless steel sheets 0.3 to 15mm thick.
    • Formats: width 360 - 2150mm, length 2000 - 8000mm

 

Surface of cold-rolled, corrosion-resistant, heat-resistant, galvanized sheets
2D Pickled Smooth With heat treatment
2B Straight and pickled Smoother than 2D
BA / 2R Straight and pickled Mirror + Foil
2E Surface without scale Rough matte
2C Surface with scale Smooth

Hot-rolled, stainless, boiler, carburizing, wear-resistant, bearing, carbon, tool, high speed plates

  • Hot-rolled sheets of carbon steel structural alloy 2 to 600mm thick.
    • Formats: width 1000 - 3000mm, length 2000 - 12000mm
  • Hot-rolled, corrosion-resistant, acid-resistant, heat-resistant and stainless steel sheets 2 to 200mm thick.
    • Formats: width 500 - 2500mm, length 2000 - 12000mm
Surface of hot-rolled, corrosion-resistant and heat-resistant sheets
1C Surface with scale rough With heat treatment
1D Pickled surface
1E Surface without scale No heat treatment
1U Surface with scale

Special surfaces of stainless and acid-resistant sheets available on request.

Special surfaces of corrosion resistant plates
3N Sheet sanded with abrasive grain 80-120
4N / 4TK Sheet sanded with abrasive grain 150-400
1K / 2K Sheets polished to a gentle gleam
1P / 2P Sheets polished for a mirror effect
1M / 2M Decorative sheets
SB Brushed sheets

Cutted elements from sheets/plates by saw, plasma, laser and waterjet

Cut or burned elements of sheet metal
Gas-plasma cut parts thickness up to 300mm
Laser cut parts thickness up to 30mm<
Saw cut elements thickness up to 1000mm
Water cut elements thickness up to 150mm

 

  • rings or discs with a hole burnt from sheets,
  • discs, full wheels burnt from sheets,
  • Forms, cubes, calcines burnt or cut from sheet metal,
  • burnt elements according to technical drawings,
  • flat bars cut from steel plates and forged blocks,

THIS WEBSITE USES COOKIES TO IMPROVE AND FACILITATE YOUR ACCESS TO THE WEBSITE AND TO KEEP STATISTICS. IF YOU CONTINUE TO USE THIS SITE, YOU AGREE THAT THE COOKIES WILL BE STORED ON YOUR DEVICE
PRIVACY POLICY
How do I disable cookies
AGREE