Drawn wire from quality steel

Steel wires are made by cold drawing (sometimes hot) from wire rods with slightly larger diameter. They are characterized by high accuracy and surface smoothness, narrow dimensional tolerances, and high strength partly obtained after the process of drawing, apart heat treatment.

The company's offer includes thin wires, very thin wires, super thin wires, medium and thick. Considering the chemical composition, wires from martensitic steels, wires made of austenitic steels and wires of ferritic steel are supplied.

Wires are supplied in coils, spools, and straight sections with specified lengths and straightness. Considering the condition of delivery, the wires are soft, semi-hard and hard. In our offer we include:


Low-alloy carbon structural wires:

Carbon grades
C4C - 1.0303 C8C - 1.0213 C10C - 1.0214 C15C - 1.0234
C20C - 1.0411 C4D - 1.0300 C7D - 1.0313 C9D - 1.0304
C10D - 1.0310 C12D - 1.0311 C15D - 1.0413 C48D - 1.0517
C50D - 1.0586 C58D - 1.0609 C60D - 1.0610 C66D - 1.0612
C68D - 1.0613 C70D - 1.0615 C72D - 1.0617 C76D - 1.0614
C78D - 1.0620 C80D - 1.0622 C82D - 1.0626 C86D - 1.0616
C88D - 1.0628 C92D - 1.0618 C2D1 - 1.1185 C3D1 - 1.1187
C4D1 - 1.1188 C3D2 - 1.1110 C5D2 - 1.1111 C8D2 - 1.1113
C10D2 - 1.1114 C12D2 - 1.1124 C15D2 - 1.1126 C18D2 - 1.1129
C2D1 - 1.1185 C3D1 - 1.1187 C4D1 - 1.1185 C3D2 - 1.1110
C5D2 - 1.1111 C8D2 - 1.1113 C10D2 - 1.1113 C12D2 - 1.1124
C15D2 - 1.1126 C46D2 - 1.1162 C48D2 - 1.1164 C58D2 - 1.1212
C60D2 - 1.1226 C62D2 - 1.1222 C66D2 - 1.1236 C70D2 - 1.1251
C72D2 - 1.1242 C78D2 - 1.1252 C82D2 - 1.1262 C86D2 - 1.1265
C88D2 - 1.1272 C92D2 - 1.1282 C15E2C - 1.1132 C17E2C - 1.1147
C20E2C - 1.1152 C35EC - 1.1172 11SMn30 - 1.0715 11SMnPb30 - 1.0718

Structural alloy wires:

Wires for hardening and carburizing
17Cr3 - 1.7016 34Cr4 - 1.7033 37Cr4 - 1.7034 41Cr4 - 1.7035
18CrNi8 - 1.5920 25CrMo4 - 1.7218 34CrMo4 - 1.7220 42CrMo4 - 1.7225
34CrNiMo6 - 1.6582 100Cr6 - 1.3505 100CrMn6 - 1.3520 17B2 - 1.5502
18B2 - 1.5503 28B2 - 1.5510 33B2 - 1.5514 38B2 - 1.5515
20MnB4 - 1.5525 32CrB4 - 1.7076 36CrB4 - 1.7077 42CrMoS4 - 1.7227
23B2 - 1.5508 18MnB4 - 1.5521 23MnB4 - 1.5535 16MnCr5 - 1.7131

Spring and tool steel wires:


Heat-resistant wires:


Stainless and acid-resistant wires - high-alloyed:


Kinds, grades and destination of wires

We offer wires:

  • corrosion-resistant, acid-resistant, and stainless, high alloyed
  • spring wires from alloy steel and carbon unalloyed steel
  • for thermal improvement and carburization
  • heat-resistant and chromium heat-resistant, chromium-nickel
  • made of precipitation strengthened, acid resistant steels
  • steel for heating and resistance elements
  • for swelling and cold extrusion
  • bearing steel and high speed HSS steel wires for drills
  • Duplex type made of high-alloy steel
  • from boiler steel for operation at elevated temperatures
  • nickel alloy and chromium alloy
  • titanium and titanium alloys
  • non-ferrous metals i.e. copper wires, brass wires, bronze wires
  • made of steel with special physical properties
  • brass, copper and other non-ferrous metals
  • tool steel, alloy steel and carbon steel
  • of alloys and special steels

Group of alloy steel available in wires:

  • CrSi, CrMn, CrMnSi, CrV, CrVSi, CrMo, CrMoV, CrW, CrWV
  • CrSiMo, CrSiMnMo, CrSiMoV, CrSiMnMoV, CrSiV, CrMnV, CrSiMnV, CrMoW, CrMoWV, CrSiTi, CrMnTi, CrSiMnTi
  • CrB, CrMnB, CrMnMoV, NiSi, NiMn, NiCu, NiMo, NiMoMn, NiMoCu, NiMoV, NiMnV
  • MnSiCu, MnSi, MnCr, MnCu, MnV, SiV, MnSiV, MnTi, SiTi, CrNiV, CrNiW, CrNiVW, CrNiMo

 

Surfaces and wire cross-sections
Round wires, cold-rolled, straight and in coils Fi 0,010 – fi 36mm tolerance H9,H10,H11

Szpule:

DIN 100

DIN 125

DIN 160

DIN 200

DIN 250

Hot drawn, dry drawn and wet drawn wires
Round, cold drawn straight wires, on rollers, spools or in coils
Round wires, ground, straight, on rollers, spools or in coils
Flat and square wires, drawn, on coils 4 x 4 - 10 x 10mm tol. H11
Hexagonal and octagonal drawn wires on coils 4 - 10mm tol. H11
Wires with cross section of regular and non-regular polygons

With regard to applications, we distinguish wires:

  • for springs for different purposes
  • for special screws, strings, staples, sheet metal screws, and rivets
  • for conveyor belts
  • for textile and construction industries
  • on braided and harp screens, string screens, woven mesh
  • for springs for automotive industry
  • for spirals and heating elements, for electric heaters
  • for needles, braids and brushes
  • for the production of fuel and air filters, for filter and catalytic sieves
  • for implants, prosthetics and jewelery
  • for the ropes for the mining and automotive industries
  • for sieves and heat-resistant mesh
  • for sorting and protective sieves for the mining industry
  • for vibration compensators

The products described above are determined by:

- Polish norms - PN-H-92603, PN-H-92604, PN-H-92611, PN-H-92612, PN-H-92600, PN-H-92601, PN-H-93003, PN-H-93222, PN-H-93223, PN-H-92610, PN-H-92336

 

- Euronorms - PN-EN 10263-1, PN-EN 10263-2, PN-EN 10263-3, PN-EN 10263-4, PN-EN 10263-5, PN-EN 10264-4, PN-EN 10270-1, PN-EN 10270-2, PN-EN 10270-3, PN-EN 10278, PN-EN 10277, EN ISO 16120, PN-EN 10016-2, PN-EN 10130, PN-EN 10016-4


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.