23MnNiCrMo5-2, 1.6541, 23MnNiCrMo5-3, 1.6540, 23MnNiMoCr5-4, 1.6758 - Structural alloy steel used for mining chain links according to PN-H-93028, PN-H-84023, DIN 17115.

 

Standards Steel Grades
Chemical Composition %
C: Mn: Si: P: S: Cr: Mo: Ni: Al: Cu: N: As:
PN
PN-H-84023/08
23GHNMA
0.20 - 0.26 1.00 - 1.25 0.15 - 0.35 <0.025 <0.025 0.4 - 0.6 0.2 - 0.3 0.4 - 0.7 0.02 - 0.07 <0.2 - -
PN 23G2NMHA
0.20 - 0.26 1.10 - 1.40 0.15 - 0.25 <0.020 <0.020 0.4 - 0.6 0.5 - 0.6 0.9 - 1.1 0.02 - 0.05 <0.2 <0.012 <0.012
DIN 23MnNiCrMo5-2 - 1.6541
0.20 - 0.26 1.10 - 1.40 <0.25 <0.02 <0.015 0.4 - 0.6 0.2 - 0.3 0.4 - 0.7 0.025 - 0.050 <0.2 <0.012 -
AFNOR 23MNCD5 - 23 MNCD 5 
0.20 - 0.26 1.10 - 1.40 0.10 - 0.35 <0.03 <0.025 0.4 - 0.6 0.2 - 0.3 0.4 - 0.7 >0.02 - - -
STAS 24 MoCrNiMn 15z - 24MoCrNiMn15z
0.21 - 0.26 1.40 - 1.70 0.17 - 0.37 <0.025 <0.020 0.4 - 0.7 0.2 - 0.3 0.4 - 0.7 0.02 - 0.05 - - -
DIN 23MnNiCrMo5-3 - 1.6540
0.20 - 0.26 1.10 - 1.40 <0.25 <0.02 <0.015 0.4 - 0.6 0.2 - 0.3 0.7 - 0.9 0.025 - 0.050 <0.2 <0.012 -
DIN 23MnNiMoCr5-4 - 1.6758
0.20 - 0.26 1.10 - 1.40 <0.25 <0.02 <0.015 0.4 - 0.6 0.5 - 0.6 0.9 - 1.1 0.025 - 0.050 <0.2 <0.012 -

 

23GHNMA - Application and specification

23GHNMA is a structural alloy steel for thermal improvement of mining chains produced by cold bending and flash welding.


Mechanical and physical properties of 23GHNMA steel

General minimum mechanical properties after thermal improvement
Tensile strength  Rm 1130 MPa
Yield point Re 1030 MPa
Elongation A5 10%
Contraction Z 45%
Impact resistance at the temp. of 20℃ 59 J/cm2
Hardness in softened state max. 187 HB
Density ρ 7,85 kg/dm³

 

Mechanical properties Properties for individual dimensions
<10mm 10 - 20mm 20 - 40mm
Tensile strength Rm > 1200 MPa > 1180 MPa > 1050 MPa
Yield point Re > 1080 MPa > 1060 MPa > 990 MPa
Elongation A5 > 12% > 10% > 10%
Contraction Z > 50% > 50% > 50%
Notch toughness KV > 60 J > 60 J > 60 J

 


In 23GHNMA and equivalents Company supply:

 


List of equivalents and other determinations of 23GHNMA steel:

23G2NMHA, 23GHNMVTA, 23G2NMHVTA, 23MnNiCrMo5-2, 1.6541, 23MNCD5, 23 MNCD 5, 24 MoCrNiMn 15z, 24MoCrNiMn15z, 23MnNiCrMo5-3, 1.6540, 23G2NMA, 23MnNiMoCr5-4, 1.6758


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.