15H, 17Cr3, 15Cr3 – case-hardening steel according to PN H-84030/02 and ISO 683-17:2014.

Standard Grade
Chemical composition %
C: Si: Mn: P: S: Cr: Ni: Cu:
PN 15H
0,12-0,18 0,17-0,37 0,5-0,8 <0.035 <0.035 0.7-1.0 <0.3 -
EN 15Cr2
0,12-0,18 0,15-0,40 0,4-0,6 <0.035 <0.035 0,4-0,7 - -
EN 17Cr3 / 1.7016
0,14-0,20 <0.4 0.6-0.9 <0.025 <0.035 0,7-1,0 - -
NF 12C3
0,09-0,15 <0,4 0.6-0.9 <0,04 <0.035 0,6-1,0 - -
JIS SCr415
0,13-0,18 0,15-0,35 0,6-0,9 <0,030 <0,030 0,9-1,2 <0,25 <0,3
GOST 15Ch
0,12-0,18 0,17-0,37 0,4-0,7 <0,035 <0,035 0,7-1,0 <0,3 <0,3
UNE F-1516
0,14-0,19 <0,4 1,0-1,3 <0,025 <0,035 0,7-0,9 - -

15H, 17Cr3, 15Cr3 – description

Steel for machine parts with low strength requirements, e.g. spindles, pins, camshafts and bushings. Weldable, machinable and cuttable steel. Weld only before carburizing. The steel is similar to 20Cr4 but has lower mechanical properties.

Physical and mechanical properties

Here You can find the mechanical properties of selected alloys. Despite their similarities, they clearly differ.

Properties Grade
PN EN EN GOST ČSN
15H 15Cr3 17Cr3 15Ch 14120
Diameter: D 15 mm 30 mm 10 mm 15 mm 30 mm
Yield strength: Re > 490 MPa > 390 MPa - > 490 MPa > 343 MPa
Tensile strength: Rm > 690 MPa 590-880 MPa < 620 MPa > 686 MPa > 588 MPa
Wydłużenie: A5 12 % 14 % - 12 % 14 %
Udarność KCU, 20°C: KCU2 70 J/cm2 - - 69 J/cm2 R3 59 J/cm2
Twardość po odprężaniu: HB < 179 HB < 202 HB < 174 HB 140-187 HB < 155 HB

Mechanical properties of 15Ch forgings

  • Thickness: < 100 mm
    • Yield strength: > 345 MPa
    • Tensile strength Rm: > 590 MPa
    • Elongation A: > 18 %
    • Hardness: 174-217 HB
    • Impact Value KCU: > 59 J/m2
    • Percent reduction of area Z: > 45 %
  • Thickness: 100-300 mm
    • Yield strength: > 345 MPa
    • Tensile strength Rm: > 590 MPa
    • Elongation A: > 17 %
    • Hardness: 174-217 HB
    • Impact Value KCU: > 54 J/m2
    • Percent reduction of area Z: > 40 %
  • Thickness: 5-10 mm
    • Yield strength: > 345 MPa
    • Tensile strength Rm: > 590 MPa
    • Elongation A: > 14 %
    • Hardness: 174-217 HB
    • Impact Value KCU: > 49 J/m2
    • Percent reduction of area Z: > 38 %
  • Thickness: 5-10 mm
    • Yield strength: > 345 MPa
    • Tensile strength Rm: > 590 MPa
    • Elongation A: > 12 %
    • Hardness: 174-217 HB
    • Impact Value KCU: > 39 J/m2
    • Percent reduction of area Z: > 33 %

Mechanical properties of 15Ch tubes

  • Wall thickness: < 10 mm
    • Tensile strength Rm: > 412 MPa
    • Elongation A: > 19 %
  • Wall thickness: > 10 mm
    • Tensile strength Rm: > 412 MPa
    • Elongation A: > 19 %
    • Hardness: < 179 HB
    • Bars, strips and reels
    • Rods
    • Wires
    • Plates

Heat treatment and plastic working

Following parameters are recommended for working and heat treatment

Treatment Grade
PN EN EN GOST ČSN
15H 15Cr3 17Cr3 15Ch 14120
Quenching Temperature 880℃ 870-900℃ 860-900℃ 880℃ 870-900℃
Cooling oil, water oil, water oil, water - water
Tempering Temperature 180℃ 150-180℃ 150-200℃ 180℃ 150-200℃
Cooling air, oil - - air, oil air

We deliver this steel alloy as:


Replacements, equivalents and other designations:

15H, 15Ch, 15Cr2, 17Cr3, 17CrS3, 12C3, 15C2, 18C3, 527A17, 527H17, 527M17, Scr21, Scr415, 15Cr9q, F-1516, 5115, G51150, 1.7016, 17ChG


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.