Structural steel for carburization 18NiCr5-4, 1.5810, 18NiCr6-4, 20NC6 for heavy-duty gears according to EN 10084.

 

StandardSteel Grade
Chemical Composition %
C:Mn:Si:P:S:Cr:Ni:Al:
EN/DIN18NiCr5-4 - 1.5810 - 18NiCr6-4
0.16 - 0.210.6 - 0.9<0.4<0.025<0.0350.9 - 1.21.2 - 1.5-
NF20NC6
0.16 - 0.210.6 - 0.90.10 - 0.35<0.030<0.0250.9 - 1.21.2 - 1.5>0.02

 

18NiCr5-4, 1.5810 - specifications and application

Carburizing steel for particularly heavy-duty gear wheels of machines and vehicles.


Mechanical properties of 18NiCr5-4, 18NiCr6-4, 1.5810

  • Hardness in +A condition: <223 HBW
  • Hardness +TH condition: 170 - 223 HBW
  • Hardness +FP condition: 156 - 207 HBW
  • Hardness in +S condition: <255 HBW

 


Heat treatment of 18NiCr5-4, 1.5810

  • Austenitization at 880 ℃ for approx. 30-35 minutes
  • Carburization at 880 - 980℃
  • Hardening at a temperature of 780 - 820℃
  • Tempering at a tempering of 150-200℃ for about 1 hour.

 


In the above mentioned grades the company provides:

 


Other replacements and equivalents

18NiCr5-4, 1.5810, 18CrNi5-4, 18NiCr6-4, 18CrNi6-4, 20NC6, F-1580, 20 NC 6.


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.