X7CrNiMoBNb16-16, 1.4986 austenitic heat-resistant steel according to EN 10088-1.

Standard Grade
Chemical composition %
C: Mn: Si: P: S: Cr: Ni: Ti: V: Mo:
EN 1.4986 - X7CrNiMoBNb16-16
0.04-0.10 0.3-0.6 0.3-0.6 <0.045 <0.030 15.5-17.5 15.5-17.5 0.4-1.2 0.05-0.10 1.6-2.0

1.4986, X7CrNiMoBNb16-16 – description

Heat-resistant steel. It contains niobium and boron along wich high amount of nickel and chromium.

Main features:

  • Heat-resistant
  • Creep-resistant
  • Contains niobium – which strengthens solution, positively affects creep-resistance and improves pitting corrosion resistance.
  • Contains boron – which improves high-temperature creep-resistance.

1.4986, X7CrNiMoBNb16-16 – physical properties

The general physical properties of the grade, as follows:

  • Density: 7.9g/cm3
  • Specific heat capacity: 460 J/kg*K
  • Modulus of elasticity (Young module): 196 GPa
  • Thermal conductivity at 20℃: 15 W/m*K
  • Linear expansion coefficient: 16.6*10-6 1/℃

Welding

This grade is classified in the group 8.1 (austenitic steel with chromium content not greater than 19%) according to ISO / TR and should be weld as such.


We deliver this steel alloy as:


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.