Alloy tool steel for hot-working X38CrMoV5-3, 1.2367, Z38CDV5-3 according to ISO 4957.

 

StandardSteel Grade
Chemical Composition %
C:Mn:Si:P:S:Cr:Mo:V:
ISO1.2367 - X38CrMoV5-3
0.35 - 0.400.3 - 0.50.3 - 0.5<0.03<0.024.8 - 5.22.7 - 3.20.4 - 0.6
DINX 38 CrMoV 5-3
0.35 - 0.400.3 - 0.60.3 - 0.5<0.035<0.0354.7 - 5.22.7 - 3.30.4 - 0.7
NFZ 38 CDV 5-3 - Z38CDV5-3
0.34 - 0.420.2 - 0.50.3 - 0.5--4.8 - 5.52.8 - 3.20.3 - 0.5
TU4Ch5MF - 4Х5МФ
0.35 - 0.400.3 - 0.60.3 - 0.5<0.035<0.0354.7 - 5.22.7 - 3.30.4 - 0.7

 

1.2367, X38CrMoV5-3 - specification and application

Tool steel for hot work with high strength properties and tempering temperature, resistance to elevated temperatures, fatigue and deformation.

It also has resistance to shock and impact when working at high temperatures and good workability.

1.2367 / X38CrMoV5-3 grade is used for the production of Aluminum, Magnesium and Zinc alloy die casting molds as well as plastics, subassemblies and die forging parts such as bushings, bolts, clamps and nuts.


Mechanical properties of X38CrMoV5-3, 1.2367

  • Hardness in +A condition: : <229 HB
  • Hardness in +A+C condition: <249 HB

 


Heat treatment of X38CrMoV5-3, 1.2367

  • Softening annealing at a temperature of 730 - 800 ℃
  • Relief annealing at a temperature of 600 - 650℃
  • Hardening at a temperature of 1030 - 1080℃
  • Tempering at a tempering of 500 - 550℃

 


In the above mentioned grade, the company provides:

 


Other indications and equivalents:

X38CrMoV5-3, X 38 CrMoV 5-3, 1.2367 ESR, X38CrMoV5-3 ESR, Z38CDV5-3, 4Ch5M3F, 4Х5М3Ф


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.