Carbon tool steel U7A/U7, C70U, C70W1, C70W2, 1.1520, 1.1620 according to PN-H-85020, DIN 17350, ISO 4957.

Standard Steel Grade
Chemical composition %
C: Mn: Si: P: S: Cr: Ni: Cu:
PN N7E
0.65 - 0.74 0.15 - 0.30 0.15 - 0.30 <0.025 <0.025 <0.15 <0.20 <0.20
PN N7
0.65 - 0.74 0.15 - 0.35 0.15 - 0.35 <0.030 <0.030 <0.20 <0.25 <0.25
GOST U7A - У7А
0.65 - 0.74 0.17 - 0.28 0.17 - 0.33 <0.025 <0.018 <0.20 <0.25 <0.25
GOST U7 - У7
0.66 - 0.73 0.20 - 0.40 0.15 - 0.35 <0.030 <0.028 <0.20 <0.25 <0.25
ISO C70W1 - C70U - 1.1520
0.65 - 0.75 0.10 - 0.40 0.10 - 0.30 <0.030 <0.030 - - -
DIN C70W2 - 1.1620
0.65 - 0.74 0.10 - 0.35 0.10 - 0.30 <0.030 <0.030 - - -

 


C70U, U7A, C70W1, C70W2 - specification and application

Deep and shallow hardening carbon steel with the lowest carbon content of N12E carbon materials. It exhibits high impact strength, shock resistance, and relatively high hardness. If we talk about its drawbacks, it is characterized by low abrasion resistance and low machinability. N7E is used for the production of tools for woodworking, soft stones, cutting boards, small die-cutting dies for hot work, smithery hammers. In some cases it can be used as a substitute for spring steels


Mechanical properties of U7A, C70W1, C70W2

  • Softened condition - hardness <187 HB
  • Hardened condition - hardness >57 HRC

Heat treatment - processes and temperatures:

  • Softening annealing at a temperature of 680 - 710 C
  • Relief annealing at a temperature of 600 - 700 C
  • Hardening at a temperature of 780 - 820 C
  • Tempering at a temperature of 170 - 190 C

In the above mentioned grades the company delivers:


Other substitutes for the N7/N7E grade

N7, N7E, C70KU, C70W1, 1.1520, C70W2, 1.1620, U7, U7A, bars C67S, TC70, S71, S72, SK7, SK65, C70E2U, У7, У7А


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.