Stainless, heat resistant and acid resistant angles

Angles are used as small bearing elements and corners in construction, parts of vehicles and machine construction. Apart from the bearing properties in the structures, the stainless steel angles combine aesthetics, elegance and not corrode.

The basic stainless steel grades are available in the form of rolled products according to standards EN 10056, DIN 1028, EN 10028-2, DIN 59370, DIN 1022, ASTM A1069. Angles in other special grades are available upon request. Depending on the purpose, the following are available:

Grades:

  • stainless, acid resistant, corrosion resistant
  • made from duplex and superduplex steel
  • heat-resistant and high-temperature creep resistance
  • from nickel and chromium-nickel alloys
  • boiler for operation at elevated temperatures
  • made from special steels

Production and surface finish:

Types of angles
Hot and cold rolled angles
  • Equal-sided angles
  • Unequal-sided angles

10 x 10 x 2 - 200 x 200 x 13mm

20 x 10 x 3 - 200 x 150 x 15mm

Cold drawn angles
  • Equal-sided angles
  • Unequal-sided angles
  • Sharp-angle angles

10 x 10 x 2 - 50 x 50 x 5mm

30 x 20 x 3 - 50 x 30 x 5mm

20 x 20 x 3 - 50 x 50 x 5mm

Laser-welded angles
  • Equal-sided angles
  • Unequal-sided angles

50 x 50 x 5 - 300 x 300 x 20mm

60 x 40 x 5 - 200 x 150 x 15mm

Grinded angles
  • K240 - K320
 
Cold-formed angles
  • from cold-rolled steel sheets
  • from hot-rolled steel sheets

Available grades of steel:

  • 1.4301, X5CrNi18-10, AISI 304,1.4307, X2CrNi18-9, AISI 304L,
  • 1.4541, 1.4878, X6CrNiTi18-10, X8CrNiTi18-10, X10CrNiTi18-10, AISI 321, AISI 321H,
  • 1.4571, X6CrNiMoTi17-12-2, AISI 316Ti,
  • 1.4404, 1.4401, X2CrNiMo17-12-2, X5CrNiMo17-12-2, AISI 316L, AISI 316,