X38CrMoV5-3, 1.2367 - tool steel
Alloy tool steel for hot-working X38CrMoV5-3, 1.2367, Z38CDV5-3 according to ISO 4957.
| Standard | Steel Grade | |||||||
|---|---|---|---|---|---|---|---|---|
| Chemical Composition % | ||||||||
| C: | Mn: | Si: | P: | S: | Cr: | Mo: | V: | |
| ISO | 1.2367 - X38CrMoV5-3 | |||||||
| 0.35 - 0.40 | 0.3 - 0.5 | 0.3 - 0.5 | <0.03 | <0.02 | 4.8 - 5.2 | 2.7 - 3.2 | 0.4 - 0.6 | |
| DIN | X 38 CrMoV 5-3 | |||||||
| 0.35 - 0.40 | 0.3 - 0.6 | 0.3 - 0.5 | <0.035 | <0.035 | 4.7 - 5.2 | 2.7 - 3.3 | 0.4 - 0.7 | |
| NF | Z 38 CDV 5-3 - Z38CDV5-3 | |||||||
| 0.34 - 0.42 | 0.2 - 0.5 | 0.3 - 0.5 | - | - | 4.8 - 5.5 | 2.8 - 3.2 | 0.3 - 0.5 | |
| TU | 4Ch5MF - 4Х5МФ | |||||||
| 0.35 - 0.40 | 0.3 - 0.6 | 0.3 - 0.5 | <0.035 | <0.035 | 4.7 - 5.2 | 2.7 - 3.3 | 0.4 - 0.7 | |
1.2367, X38CrMoV5-3 - specification and application
Tool steel for hot work with high strength properties and tempering temperature, resistance to elevated temperatures, fatigue and deformation.
It also has resistance to shock and impact when working at high temperatures and good workability.
1.2367 / X38CrMoV5-3 grade is used for the production of Aluminum, Magnesium and Zinc alloy die casting molds as well as plastics, subassemblies and die forging parts such as bushings, bolts, clamps and nuts.
Mechanical properties of X38CrMoV5-3, 1.2367
- Hardness in +A condition: : <229 HB
- Hardness in +A+C condition: <249 HB
Heat treatment of X38CrMoV5-3, 1.2367
- Softening annealing at a temperature of 730 - 800 ℃
- Relief annealing at a temperature of 600 - 650℃
- Hardening at a temperature of 1030 - 1080℃
- Tempering at a tempering of 500 - 550℃
In the above mentioned grade, the company provides:
Substitutes, equivalents and other species designations
Need help? Contact us!
Call or send a message, and our representative
will contact you within 24 hours!
Write
Call