X32CrMoCoV3-3-3, 1.2885 - Tool steel for Hot work

Hot-work tool steel WLK, X32CrMoCoV3-3-3, 1.2885 according to PN-86/H-85021.

Standard Steel Grade
Chemical composition %
C: Mn: Si: P: S: Cr: Mo: V: Co: Cu:
PN WLK
0.30 - 0.40 0.25 - 0.50 0.30 - 0.60 <0.030 <0.030 2.50 - 3.00 2.50 - 3.00 0.40 - 0.60 2.80 - 3.30 <0.30
DIN X32CrMoCoV3-3-3 - 1.2885
0.28 - 0.35 0.15 - 0.45 0.10 - 0.40 <0.030 <0.030 2.70 - 3.20 2.60 - 3.00 0.40 - 0.70 2.50 - 3.00 -
GOST 3Ch3M3K3F - 3Х3М3К3Ф
0.28 - 0.35 0.15 - 0.45 0.10 - 0.40 <0.030 <0.030 2.70 - 3.20 2.60 - 3.00 0.40 - 0.70 2.50 - 3.00 -
BS BH10A
0.30 - 0.40 <0.4 0.75 - 1.10 - - 2.80 - 3.20 2.65 - 2.95 0.30 - 1.10 2.80 - 3.20 <0.20
UNE 32CrMoCoV12
0.28 - 0.35 0.15 - 0.45 0.10 - 0.40 <0.030 <0.020 2.70 - 3.20 2.60 - 3.00 0.40 - 0.70 2.50 - 3.50 -
UNI 30CrMoCoV123012KU
0.26 - 0.34 0.30 - 0.60 0.10 - 0.40 - - 2.60 - 3.40 2.60 - 3.40 0.70 - 1.10 2.60 - 3.40 -

WLK, X32CrMoCoV3-3-3, 1.2885 - specification and application

Alloy tool steel with high hardenability, high resistance to tempering, load and high hardness at elevated temperatures. The grade is distinguished by high content of Cobalt in its chemical composition. Steel is used for high speed tools for automatic forging and upset forging of bolts, nuts, bolt heads and rivets. The material is used to manufacture die inserts, press and forge stamps, as well as tools for forging rolling bearing rings.

Mechanical properties of WLK, 1.2885, X32CrMoCoV3-3-3

  • Hardness in softening annealed condition <241 HB
  • Hardness after hardening 53.5 HRC
  • Hardness after tempering at temperature:
    • 300C = 51.5 HRC
    • 350C = 51.5 HRC
    • 400C = 52.0 HRC
    • 450C = 52.5 HRC
    • 500C = 53.0 HRC
    • 550C = 53.5 HRC
    • 600C = 51.5 HRC
  • Linear expansion coefficient α: 12,4 * 10-6 K-1
  • Thermal conductivity λ: 37 W*m-1*K-1

Heat treatment - processes and temperatures:

  • Softening annealing at 740 - 770C with cooling in furnace
  • Relief annealing at a temperature of 600 - 700C with cooling in furnace
  • Nitriding at a temperature of 470 - 550C
  • Hardening at a temperature of 1020 - 1040C with cooling in oil
  • Tempering at a temperature of 500 - 600C

In the above mentioned grades the company delivers:

Substitutes, equivalents and other species designations

WLK
30 CrMoCoV12 30 12 KU
30CrMoCoV12-30-12 KU
32CrMoCoV12
32 CrMoCoV 12
1.2885 EFS
ESR
W321
BH10A
BH 10 A
UD30
3Ch3M3K3F
USMoCo
WMoCo
X32CrMoCoV3-3-3
30DCKV28
AISI H10

Need help? Contact us!

Call or send a message, and our representative
will contact you within 24 hours!

We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie preferences
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.