1.4003, X2CrNi12, AISI 410L - stainless steel
Stainless ferritic steel X2CrNi12, 1.4003, AISI 410L with the addition of Nickel and Nitrogen according to EN 10088-1.
| Standard | Steel Grade | |||||||
|---|---|---|---|---|---|---|---|---|
| Chemical Composition % | ||||||||
| C: | Mn: | Si: | P: | S: | Cr: | Ni: | N: | |
| EN | X2CrNi12 - X 2 CrNi 12 - 1.4003 | |||||||
| <0.03 | <1.5 | <1.0 | <0.04 | <0.030 | 10.5 - 12.5 | 0.3 - 1.0 | <0.03 | |
| ASTM | UNS S40977 | |||||||
| <0.03 | <1.5 | <1.0 | <0.04 | <0.015 | 10.5 - 12.5 | 0.3 - 1.0 | <0.03 | |
| JIS | G4303 - SUS 410L - SUS 410 L | |||||||
| <0.03 | <1.0 | <1.0 | <0.04 | <0.030 | 11.0 - 13.5 | <0.6 | - | |
Specifications and application
X2CrNi12 is a stainless steel with ferritic structure, which chemical composition from 0H13, X6Cr13, 1.4006, AISI 410S deviates from the original by a small addition of Nickel, and even more limited content of Carbon. Chromium at a concentration of approx. 12% allows users to use the material as a building material in non-aggressive environments, including decorative purpose.
Steel does not show resistance to acids, chlorides, salts or marine environments to such an advanced extent as austenitic steels. For applications as a corrosion-resistant material, coating of the material and proper surface treatment is required. The products can be used to produce components and decorative elements in the construction industry, or parts of vehicles in the communication and automotive industries.
Steel also found in the food, mining and sugar industries. .In addition, X2CrNi12 is easily weldable, has relatively good mechanical properties in annealed condition +A, at room and elevated temperatures.
Mechanical properties of X2CrNi12, 1.4003 in annealed condition +A
- Tensile strength, Rm: 450 - 650 MPa
- The yield point, Re: > 250 MPa
- Elongation, A:> 18%
- Hardness, HB: <200
- Module of elasticity, E: 220 GPa
- Linear expansion coefficient, α20℃: 10,4 * 10-6 K-1
- Thermal capacity, cp = 430 J * kg-1 * K-1
- Thermal conductivity, λ = 25 W * m-1 * K-1
- Specific resistance, Ω: 0,6 mkOhm * m
Mechanical properties at elevated temperatures
| Properties | Temperature | ||||
|---|---|---|---|---|---|
| 100℃ | 200℃ | 300℃ | 400℃ | 500℃ | |
| Linear expansion coefficient, α (*10-6 K-1) | 10,4 | 10,8 | 11,2 | 11,6 | 11,9 |
| The yield point, Rp0,2 (MPa) | >240 | >220 | >210 | - | - |
| Modulus of elasticity, E (GPa) | 215 | 210 | 205 | 195 | - |
Heat treatment - processes and temperature
- Rolling and forging at 1100 - 800℃ with cooling in the air
- Annealing + A at 680 - 760℃ with cooling in water or air
In the aforementioned grades we supply companies with:
Substitutes, equivalents and other species designations
Need help? Contact us!
Call or send a message, and our representative
will contact you within 24 hours!
Write
Call