X210CrW12, 1.2436, X210Cr12, 1.2080
X210CrW12, 1.2436, X210Cr12, 1.2080 - high carbon tool steel for cold working according to ISO 4957.
| Standard | Steel Grade | |||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Chemical Composition % | ||||||||||
| C: | Mn: | Si: | P: | S: | Cr: | W: | V: | Cu: | ||
| ISO | X210CrW12 - 1.2436 | |||||||||
| 2.0 - 2.3 | 0.3 - 0.6 | 0.1 - 0.4 | <0.03 | <0.03 | 11.0 - 13.0 | 0.6 - 0.8 | - | - | ||
| ISO | X210Cr12 - 1.2080 | |||||||||
| 1.9 - 2.2 | 0.2 - 0.6 | 0.1 - 0.6 | <0.03 | <0.03 | 11.0 - 13.0 | - | - | - | ||
| PN | NC11 | |||||||||
| 1.8 - 2.1 | 0.15 - 0.45 | 0.15 - 0.40 | <0.03 | <0.03 | 11.0 - 13.0 | - | - | <0.35 | ||
| NF | Z200C12 | |||||||||
| 1.9 - 2.2 | 0.15 - 0.45 | 0.1 - 0.4 | - | - | 11.0 - 13.0 | - | - | - | ||
| NF | Z210CW12-01 | |||||||||
| 2.0 - 2.3 | 0.15 - 0.45 | 0.1 - 0.4 | - | - | 11.0 - 13.0 | 0.6 - 0.8 | - | - | ||
| ASTM | AISI D3 - UNS T30403 | |||||||||
| 2.00 - 2.35 | 0.1 - 0.6 | 0.1 - 0.6 | <0.03 | <0.03 | 11.0 - 13.5 | <1.0 | <1.0 | - | ||
| GOST | Ch12 - Х12 | |||||||||
| 2.0 - 2.2 | 0.15 - 0.45 | 0.1 - 0.4 | <0.03 | <0.03 | 11.5 - 13.0 | <0.2 | <0.15 | <0.3 | ||
| TU | Ch12V - Х12В | |||||||||
| 2.00 - 2.25 | 0.15 - 0.45 | 0.1 - 0.4 | <0.03 | <0.03 | 11.0 - 12.0 | 0.6 - 0.8 | - | - | ||
X210CrW12, 1.2436 - specifications and applications
High carbon tool chromium steel with the addition of tungsten with a higher carbon content than NC11. It is characterized by low ductility and brittleness, excellent abrasion resistance and very high hardness. It is mainly used for tools for punching, cutting and stamping metal sheets, as well as for the production of haulers, cutters, reamers, gauges, drawing dies and disc knives. The addition of tungsten improves the hardenability of the grade, which results in the possibility of higher hardness.
Mechanical properties of X210CrW12, 1.2436
- Hardness in +A delivery condition: <255 HB
- Hardness in +A +C delivery condition: <275 HB
- Theoretical hardness after hardening and tempering of small diameters at temperatures:
- 100℃ = 64.0 HRC
- 200℃ = 62.5 HRC
- 300℃ = 61.0 HRC
- 400℃ = 59.0 HRC
- 500℃ = 57.0 HRC
- 600℃ = 55.0 HRC
Heat treatment
- Softening annealing at 800 - 850℃
- Relief annealing at 600 - 650℃
- Hardening at 960 - 980℃ with cooling in oil at 500 - 550℃.
- Tempering at 200-500℃, at your choice
In the above mentioned grades the company offers:
Substitutes, equivalents and other species designations
Need help? Contact us!
Call or send a message, and our representative
will contact you within 24 hours!
Write
Call