C75S, 1.1248, C75 - spring steel

sizes Carbon steel spring cutted sheets, belts, and pieces - MORE DETAILS
Thicnkess: 0,05 - 4,00mm
width: standard 300mm (100 - 500mm)
lenght: standard 1000mm (100 - 5000mm)
Rm: 1100-1300 | 1300-1500 | 1500-1700 N/mm2
FULL DIMENSIONAL LIST - CLICK HERE

C75S, 1.1248, AISI 1075, XC70 - Carbon low-alloy structural steel for oil hardening for lightweight springs according to PN-74/H-84032 and EN 10132-4.

Standards Steel Grades
Chemical Composition %
C: Mn: Si: P: S: Cr: Mo: Ni: Cu:
PN 75
0.72 - 0.80 0.50 - 0.80 0.17 - 0.37 <0.040 <0.040 <0.30 - <0.30 <0.25
EN / DIN C75S - C 75 S - 1.1248 - 1248
0.70 - 0.80 0.60 - 0.90 0.15 - 0.35 <0.025 <0.025 <0.40 <0.10 <0.40 -
AFNOR XC 75 - XC75
0.70 - 0.80 0.40 - 0.70 0.15 - 0.30 <0.035 <0.025 - - - -
DIN C75 - C 75 - 1.0605
0.70 - 0.80 0.60 - 0.80 0.15 - 0.35 <0.045 <0.045 - - - -
GOST 75
0.72 - 0.80 0.30 - 0.70 0.17 - 0.37 <0.035 <0.035 <0.15 - <0.15 <0.20
DIN Ck 75 - Ck75
0.70 - 0.80 0.60 - 0.80 0.15 - 0.35 <0.035 <0.035 - - - -
DIN 75Cr1 - 75 Cr 1 - 1.2003 - 2003
0.70 - 0.80 0.60 - 0.80 0.25 - 0.50 <0.03 <0.03 0.30 - 0.40 - - -
BS CS80
0.75 - 0.85 0.50 - 0.90 0.05 - 0.35 <0.045 <0.045 - - - -
JIS S 75 CM - S75CM
0.70 - 0.80 0.60 - 0.90 0.15 - 0.35 <0.030 <0.035 <0.20 - <0.20 <0.30
STAS OLC 75A - OLC75A
0.70 - 0.80 0.50 - 0.80 0.17 - 0.37 <0.040 <0.040 <0.30 - <0.30 <0.25
ČSN / STN 12081 - 12 081
0.70 - 0.80 0.40 - 0.65 <0.35 <0.035 <0.035 - - - -
ASTM AISI 1075
0.70 - 0.80 0.40 - 0.70 - <0.040 <0.050 - - - -

Steel C75S, 1.1248, 75Cr1, 1.2003 grade - specification and application

75 steel - C75S - Carbon spring steel with low hardening capacity for lightweight springs for oil hardening. It is characterized by resistance to abrasion and high strength. Used for low-loaded springs and springs, spring parts, clock springs, saws for cutting stones in the form of tapes and sheets.

As a constructional steel, it is used for medium-weight machine parts such as bolts and bucket links, rolls, molding boards, agricultural machinery parts, press plates and ball mills, press rods, and briquette presses. Non-weldable steel, resistant to temper embrittlement, prone to decarburization and oxidation during heat treatment.

Mechanical and physical properties C75S, 1.1248

Mechanical and physical properties
Heat-treated state C75S +QT
Tensile strength Rm 1200 - 1900 MPa
Hardness HV HRC 370 - 580 HV 38.5 - 54.0 HRC
Cold-rolled state C75S +CR
Tensile strength Rm ≤ 1170 MPa
Hardness HV ≤ 320 HV
Soft state after smoothing rolling C75S +A+LC
Tensile strength Rm ≤ 640 MPa
Yield point Re ≤ 510 MPa
Elongation A > 15%
Hardness HV HRC < 200 HV < 93 HB
General properties of C75S grade
Tensile strength Rm ≥ 1080 MPa
Yield point Re ≥ 880 MPa
Hardness in the raw condition ≤ 285 HB
Hardness in softened condition ≤ 241 HB
Contraction Z ≥ 30%
Elongation A ≥ 9%
Density ρ ~7.85 kg/dm³
Linear Expansion Factor α20-100℃ ~11.4 ⋅ 10⁻⁶ K⁻¹
Heat capacity cp 20-100℃ ~483 J ⋅ ​kg⁻¹ K⁻¹
Heat conductivity λ20℃ 49.81 W ⋅ m⁻¹ K⁻¹

Heat treatment of C75S, C75, 1.1248 steel - process and temperatures

Heat treatment
Process Cooling Temperatures
Normalizing annealing in air 790 - 820℃
Softening annealing 660 - 700℃
Hardening in oil 810 - 830℃
Tempering in air 460 - 500℃

Substitutes, equivalents and other species designations

gat. 75
C75S
C 75 S
1.1248
1248
XC 75
XC75
C75
C 75
1.0605
75
CS80
S 75 CM
S75CM
OLC 75A
OLC75A
ČSN 12081
ČSN 12 081
AISI 1075
75Cr1
75 Cr 1
1.2003
2003

Need help? Contact us!

Call or send a message, and our representative
will contact you within 24 hours!

We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie preferences
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.