C100S, 1.1274, AISI 1095 - spring steel

sizes Carbon steel spring cutted sheets, belts, and pieces - MORE DETAILS
Thicnkess: 0,005 - 2,00mm
width: standard 300mm (100 - 500mm)
lenght: standard 1000mm (100 - 5000mm)
Rm: 1600-1900 | 1800-2000 | 2000-2000 N/mm2
FULL DIMENSIONAL LIST - CLICK HERE

C100S, 1.1274, AISI 1095 - Spring non-alloyed carbon steel for heat treatment - hardening in oil, according to EN 10132-4 i EN 10271.

Standard Steel Grade
Chemical Composition %
C: Mn: Si: P: S: Cr: Mo: Ni: Al: Cu:
EN/DIN C100S - 1.1274 - C 100 S - C101E - C 101 E
0.95 - 1.05 0.30 - 0.60 0.15 - 0.35 <0.025 <0.025 <0.40 <0.10 <0.40 - -
EN 2CS100 - 2 CS 100
0.95 - 1.05 0.45 - 0.60 0.15 - 0.40 <0.035 <0.035 - - - - -
AFNOR C100RR - C 100 RR - XC100
0.95 - 1.05 0.30 - 0.60 0.15 - 0.30 <0.025 <0.020 <0.30 <0.10 <0.40 <0.03 -
AFNOR XC 100 - E100 - E 100
0.95 - 1.05 0.25 - 0.45 0.15 - 0.30 <0.030 <0.025 - - - - -
DIN / LW Ck 101 - Ck101
0.95 - 1.05 0.40 - 0.60 0.15 - 0.35 <0.035 <0.035 - - - - -
BS CS95 - CS 95 - HS95 - HS 95
0.90 - 1.00 0.30 - 0.60 0.05 - 0.35 <0.04 <0.04 - - - - -
IS 98C6 Grade 8
0.90 - 1.05 0.50 - 0.80 0.10 - 0.35 <0.05 <0.05 - - - - -
ISO CS95
0.90 - 1.04 0.30 - 0.60 0.10 - 0.35 <0.035 <0.030 - - - - -
UNI C100 - C 100 - E4 - E 4
0.95 - 1.05 0.40 - 0.60 0.15 - 0.40 <0.035 <0.035 - - - - -
JIS SK95-CSP - SK4-CSP
0.90 - 1.10 <0.50 <0.35 <0.030 <0.030 <0.30 - - - <0.25
UNE C 102 - C102 - A-5117 - F-5117
0.95 - 1.09 <0.35 <0.35 <0.030 <0.030 - - - - -
STAS OSC 10 - OSC10
0.95 - 1.04 0.10 - 0.35 0.15 - 0.35 <0.030 <0.025 <0.20 - <0.25 - <0.25
AISI AISI 1095
0.90 - 1.03 0.30 - 0.50 - <0.040 <0.050 - - - - -

Steel C100S (1.1274) - specification and application

Low-alloy carbon steel for thermal improvement by oil hardening available in strips and thin cold-rolled sheets used for springs and leaf springs with small cross-sections. It is characterized by low hardenability, abrasion resistance and decarburization and oxidation tendency during heat treatment.

C100S steel products and its equivalents do not show resistance to atmospheric corrosion, and after heat treatment get tempered martensite structure. Carbon spring steels are delivered in various hardening and soft condition variants.

Steel used for spring washers, spring elements, feeler gauges, and other loaded parts requiring high elasticity and tensile strength.

Mechanical properties of C100S (1.1274) steel

Mechanical properties
The softened condition after smoothing rolling C100S + +A+LC
Tensile strength Rm < 690 MPa
The yield point Re < 550 MPa
Elongation A > 13%
Hardness HV HRB < 220 HV < 95 HRB
Cold-rolled condition C100S +CR
Tensile strength Rm < 1200 MPa
Hardness HV < 325 HV
Heat-treated condition +QT
Tensile strength Rm 1200 - 2100 MPa
Hardness HV HRC 370 - 630 HV 38.5 - 57.0 HRC

Substitutes, equivalents and other species designations

C100S
1.1274
C 100 S
C101E
C 101 E
2CS100
2 CS 100
C100RR
C 100 RR
XC100
XC 100
E100
E 100
Ck 101
Ck101
CS95
CS 95
HS95
HS 95
98C6 Grade 8
C100
C 100
E4
E 4
SK95-CSP
SK4-CSP
C 102
C102
A-5117
F-5117
OSC 10
OSC10
AISI 1095

Need help? Contact us!

Call or send a message, and our representative
will contact you within 24 hours!

We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie preferences
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.