Capillary tubes

Capillary tubes

Capillary tubes are special, precision-made, high quality metallurgical products of circular profile, obtained by cold drawing. Unlike standard hot and cold made seamless pipes, they are characterized by extremely small walls and diameters with a particularly narrow dimension.

The capillary tubes, apart from their small dimensions, are characterized by much smaller deviations of the straightness, precision of the surface itself, the length and the ends of the product. The best visual example that will stimulate the reader's imagination is the needle present in everyday medicine.

Capillary tubes are most often produced from stainless steel, acid resistant, heat resistant and creep resistant, special alloys, nickel, titanium and other non-ferrous metals. They are used for the production of pressure equipment and systems, measuring technology equipment, specialized food processing equipment in the food and nitrogen industry, ship construction, parts responsible for furnaces and boilers, and hydrogen discharge systems.

The outer diameter range of capillary tubes should be closed in the range of 0.30 - 20.00 mm, while the wall thickness range is between 0.10 - 6.00 mm. The use of capillary tubes can be found in the engineering, pharmacological, aerospace, petrochemical and chemical industries, and in the energy, food, cryogenic and machine industries.

We provide - Capillary tubes in coils or in straight sections, cut to size according to customer specifications, with a variety of surface finishes and ends:

  • Diameters: 0.30 - 25.00mm
  • Wall thickness: 0.10 - 6.00mm

Capillary tubes, heat-resistant capillaries - Grades

Heat resistant capillary tubes

Capillary tubes, nickel and titanium alloys capillary

Capillary tube in Special Alloys
2.4360
  • Alloy 400
  • NiCu30Fe
  • NiCu30Mn3Ti
  • UNS N04400
2.4068
  • Alloy 201
  • LC-Ni99
  • UNS N02201
2.4602
  • Alloy C22
  • NiCr21Mo14W
  • NiCr21Mo13W3
  • UNS N06022
2.4605
  • Alloy 59
  • NiCr23Mo16Al
  • UNS N06059
2.4610
  • Alloy C4
  • NiMo16Cr16Ti
  • NiCr16Mo15Ti
  • UNS N06455
2.4816
  • Alloy 600
  • NiCr15Fe8NiCr15Fe
  • UNS N06600
2.4819
  • Alloy C276
  • NiMo16Cr15W
  • CrNiMo15-60-16
  • UNS N10276
2.4851
  • Alloy 601
  • NiCr23Fe
  • NiCr23Fe15Al
  • UNS N06601
2.4856
  • Alloy 625
  • NiCr22Mo9Nb
  • UNS N06625
2.4858
  • Alloy 825
  • NiCr21MoCrNiMo21-42-3
  • UNS N08825
3.7025
  • Titanium Grade 1
  • Ti Gr. 1
  • UNS R50250
We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie preferences
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.