Cold-rolled steel strips
Cold-rolled and hot-rolled strips
Hot- and cold-rolled strips are gaining popularity in various industries. They are increasingly being implemented in engineering projects, through a fairly large number of small component manufacturers, parts and machine components.
By making the right choice to buy steel strips, we reduce the amount of waste produced, thereby saving time and space. With a constant focus on the needs and requirements of our customers, we have created a unique offer where you can find strips such as:
- stainless corrosion-resistant strips
- carbon spring strips C55S, C67S, C75S, C85S, C90S, C100S, C125S
- alloy spring strips
- for hardening and carburizing
- for work at elevated temperatures
- made of high-speed steel
- made of tool steel for cold working
- made of carbon tool steel
- made of martensitic stainless steel
- low carbon for stamping
- low-alloy for cold working
- heat-resistant and high-temperature creep resistance
- structural carbon hardened
- Nirosta stripes
- for tanks and pressure equipment
- chrome plated, steel covered with a layer of blue chrome
- coated with copper and brass
- nickel plated steel
Carbon and alloy spring strips
Construction alloy strips for carburizing/thermal improvement
- 1.1121
- 1.1141
- 1.1151
- 1.1181
- 1.1186
- 1.1191
- 1.1206
- 1.1203
- 1.1221
- 1.7218
- 1.7220
- 1.7225
- 1.7228
- 1.7003
- 1.7035
- 1.7015
- 1.7016
- 1.7131
- 1.7147
- 1.5530
- 1.5528
- 1.5533
- 1.5529
- 1.5531
Tool steel strips
Stainless and acid-resistant strips
- X6Cr17
- X6CrMo17-1
- X2CrMoTi18-2
- X2CrTiNb18
- X3CrNb17
- X2CrTi12
- X2CrTi17
- X12Cr13
- X20Cr13
- X30Cr13
- X46Cr13
- X17CrNi16-2
- X15CrNiSi25-21
- X15CrNiSi20-12
- X5CrNi18-10
- X4CrNi18-12
- X2CrNi19-11
- X2CrNi18-9
- X10CrNi18-8
- X5CrNiMo17-12-2
- X2CrNiMo17-12-2
- X2CrNiMo18-14-3
- X3CrNiMo17-13-3
- X2CrNiMoN17-13-5
- X1NiCrMoCu25-20-5
- X2CrNiMoN17-13-3
- X6CrNiTi18-10
- X8CrNiTi18-10
- X7CrNiAl17-7
- X6CrNiMoTi17-12-2
- X2CriMoN22-5-3
Cold-rolled and hot-rolled strips - type of surfaces and edges:
| Steel strips | ||||
|---|---|---|---|---|
| Hot-rolled strips | 2D, 2B, BA / 2R, 2E, 2C, 2H, 2Q | slit | Thickness: 0,025 - 5,50mm width: 2 - 700mm | |
| MA, RL, RM, RR | Rounded | |||
| Deburred | ||||
| Cold-rolled strips | MB, RL, RM | Cold shut | ||
| Beveled on one side | ||||
| MC, RN | Bevel cut on both sides | |||
| Grooved | ||||
| Belts and sheets cutted from strips | Grinded strips | Chamferred | ||
| Brushed strips | Rounded under the agreed angle | |||
| Polished strips | ||||
The above described products in the form of cold-rolled tapes are in accordance with:
- Polish Norms - PN-H-92326, PN-H-92327, PN-H-92329, PN-H-92330, PN-H-92331, PN-H-92332, PN-H-92335, PN-H-84023.03, PN-H-92336.
- Euronorms - PN-EN 10130, PN-EN 10132-2, PN-EN 10132-3, PN-EN 10132-4, PN-EN 10139, PN-EN 10151, PN-EN 10205, PN-EN 10207, PN-EN 10265, PN-EN 10327, PN-EN 10333, PN-EN 10334, PN-EN 10335, PN-EN 10336.