50CrMo4, 1.7228 - alloy steel

Chromium-molybdenum machine construction steel 50CrMo4/1.7228 for thermal improvement in accordance with EN 10083-1.

Standards Steel Grades
Chemical Composition %
C: Mn: Si: P: S: Cr: Mo: Ni: Cu:
EN 50CrMo4 - 1.7228
0.46 - 0.54 0.5 - 0.8 <0.4 <0.025 <0.035 0.9 - 1.2 0.15 - 0.30 - -
PN 50H
0.47 - 0.55 0.5 - 0.8 0.17 - 0.37 <0.035 <0.035 0.8 - 1.1 - <0.3 -
DIN 48CrMo4 - 48 CrMo 4 - 1.3565
0.46 - 0.52 0.5 - 0.8 <0.4 <0.025 <0.035 0.9 - 1.2 0.15 - 0.30 - <0.3
GOST 50ChM - 50KhM - 50ХМ
0.46 - 0.54 0.5 - 0.8 <0.4 <0.025 <0.035 0.9 - 1.2 0.15 - 0.35 - -
DIN 50 CrMo 4
0.46 - 0.54 0.5 - 0.8 <0.4 <0.035 <0.035 0.9 - 1.2 0.15 - 0.30 - -
AFNOR 50CD4 - 50 CD 4
0.46 - 0.54 0.5 - 0.8 <0.4 <0.025 <0.035 0.9 - 1.2 0.15 - 0.30 - -
ASTM AISI 4150
0.48 - 0.53 0.75 - 1.00 0.75 - 1.00 <0.035 <0.040 0.8 - 1.1 0.15 - 0.25 - -

Steel 50CrMo4 - Specification and application

50CrMo4 is steel related to 42CrMo4, 34CrMo4 as well as 25CrMo4. These standards, apart from practically the same concentration of Chromium and Molybdenum, are distinguished by much lower average carbon content in the chemical composition. 50CrMo4 is one of the last grades that is classified as structural steel for thermal improvement and its only similar steel grade is 50H - not containing Molybdenum.

Products with a particular composition are dedicated for vehicles and machines that require high hardness and are subject to strong bending, twisting, abrasion and wear loads. They have a higher yield point than other HM steels.

They are used as semi-finished products for the manufacture of components such as crankshafts, cogwheels, heavy-duty axles, gears, valves, heavy-duty screws, thrust rollers, guides, articulated joints, thrust rings, bolts or bushes.

For some applications, the steel may exhibit good spring properties. Simple yet proven chemical composition allows for easy welding of parts and mechanical cutting.

50CrMo4 - General mechanical properties

  • Tensile strength Rm = 1100 - 1300 MPa
  • Yield point Re > 900 MPa
  • Notch toughness KV > 30 J
  • Elongation, A > 9%
  • Contraction, Z > 40%

Heat treatment - processes, temperatures and cooling

  • Softening annealing at 680 - 720℃
  • Normalizing at 840 - 880℃
  • Hardening in oil at 820 - 860℃
  • Tempering at 540 - 680℃

Virgamet company in the beforementioned grade provides:

Substitutes, equivalents and other species designations

50 CrMo 4
1.7228
AISI 4150
SCM5
50CrMo4H
50CrMo4HH
50CrMo4HL
50ChM
50KhM
50ХМ
48CrMo4
48 CrMo 4
1.3565
SCM 445
50CD4
50 CD 4
50H

Need help? Contact us!

Call or send a message, and our representative
will contact you within 24 hours!

We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie preferences
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.