30HGSNA, 30HGSN2A - alloy structural steel

30HGSNA, 30HGSN2A - alloy steel for heat treatment in accordance with PN-H-84035, GOST 4543-71.

Standard Steel Grade
Chemical composition %
C: Mn: Si: P: S: Cr: Ni: Mo: V: Ti: Cu:
PN 30HGSNA
0.27 - 0.34 1.0 - 1.3 0.9 - 1.2 <0.030 <0.025 0.9 - 1.2 1.4 - 1.8 - - - <0.20
GOST 30HGSN2A - 30XГСН2А
0.27 - 0.34 1.0 - 1.3 0.9 - 1.2 <0.030 <0.025 0.9 - 1.2 1.4 - 1.8 <0.11 <0.05 <0.03 <0.30
GOST 30HGSN2A-Sh - 30XГCН2А-Ш
0.27 - 0.34 1.0 - 1.3 0.9 - 1.2 <0.025 <0.015 0.9 - 1.2 1.4 - 1.8 <0.15 <0.05 <0.03 <0.25
GOST 30HGSN2A-VD - 30XГCН2А-ВД
0.27 - 0.34 1.0 - 1.3 0.9 - 1.2 <0.025 <0.015 0.9 - 1.2 1.4 - 1.8 <0.11 <0.05 <0.03 <0.30
TU 30HGSN2MA - 30XГCН2МА
0.27 - 0.34 1.0 - 1.3 0.9 - 1.2 <0.025 <0.025 0.9 - 1.2 1.4 - 1.8 0.30 - 0.45 - - <0.25
TU 30HGSN2MA-VD - 30XГCН2МА-ВД
0.28 - 0.34 0.8 - 1.2 0.9 - 1.2 <0.025 <0.005 0.8 - 1.1 1.8 - 2.1 0.35 - 0.45 - - -

30HGSNA, 30HGSN2A - specification and application

A structural alloy grade similar to 30HGSA, enriched with nickel for better plasticity and significantly higher mechanical properties. Used mainly on extremely loaded shafts and parts of aircraft engines. It is characterized by high hardenability, high tensile strength, lack of tempering brittleness and extremely high yield strength. 30HGSNA is hardened in oil, tempers at low and medium temperatures, achieving the best properties up to 100mm diameter. The products are not suitable for welding.

Mechanical properties 30HGSN2A - GOST 4543

  • Tensile strength, Rm >1617 N/mm2
  • Yield strength, Re: >1375 N/mm2
  • Elongation, A: >9%
  • Necking, Z: >45%
  • Impact energy, KU2: >59 J
  • Hardness, HB: >450
  • Linear expansion coefficient: 11,5 * 10-6 K-1

Mechanical properties of tubes 30HGSN2A - GOST 21729-76

  • Tensile strength, Rm: >588 N/mm2
  • Elongation, A: >15%

Mechanical properties of sheets and plates 30HGSNA - GOST 11269, GOST 11268:

  • Tensile strength, Rm: >1570 N/mm2
  • Elongation, A: >9%
  • Impact test, KCU: >59 J

Heat treatment - processes and temperatures:

  • Softening annealing at a temperature of 640-680°C
  • Softening annealing at a temperature of 840-860°C
  • Hardening in oil at 900°C
  • Tempering in the temperature range 200-300°C (260)

In the above mentioned grades the company delivers:

Substitutes, equivalents and other species designations

30HGSNA
30ChGSNA
30ChGSN2A
30HGSN2A
CSN STN 16532
30ХГСН2А-Ш
30HGSN2A-Sh
30ХГСН2А-ВД
30HGSN2A-VD
30ХГСН2МА-ВД
30HGSN2MA-VD

Need help? Contact us!

Call or send a message, and our representative
will contact you within 24 hours!

We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie preferences
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.