1.4570, X6CrNiCuS18-9-2, UNS S30330 - stainless steel

1.4570, X6CrNiCuS18-9-2, UNS S30330 - stainless steel, data according to EN 10088-3:2014

Standard Grade
Chemical composition %
C: Si: Mn: P: S: Cr: Mo: Ni: Cu: N: Se:
EN 1.4570 - X6CrNiCuS18-9-2
<0.08 <1.0 <2.0 <0.045 0.15 - 0.30 17.0-19.0 <0.6 8.0 - 10.0 1.4 - 1.8 <0.11 -
ASTM AISI 303Cu - UNS S30330
<0.15 <1.0 <2.0 <0.15 <0.15 17.0 - 19.0 - 6.0 - 10.0 2.5 - 4.0 - <0.1
JIS SUS303Cu
<0.15 <1.0 <3.0 <0.2 >0.15 17.0 - 19.0 <0.6 8.0 - 10.0 1.5 - 3.5 - -

1.4570, X6CrNiCuS18-9-2, AISI 303Cu – description

Copper-containing variant of chrome-nickel austenitic steel. Used in the chemical industry, in fuel processing and food processing plants for heat exchangers, coolers, tanks, vessels, pump elements, etc.

The alloying addition of copper increases resistance to corrosion in acidic and non-oxidized environments (sulphuric acid, phosphoric acid) and improves deformability. The alloy is not resistant to intergranular corrosion.

Welding does not require pre-heating.

Physical and mechanical properties

1.4570 - general physical and mechanical properties:

  • Density: 7.9 g/cm3
  • Young's modulus E: 200 GPa
  • Tensile strength Rm: 500-710 MPa
  • Yield strength Re: > 185 MPa
  • Elongation A: > 35 %
  • Hardness HB: < 215

Young's modulus (E) in given temperature:

  • In ambient temperature: - 200 GPa
  • Testing temperature: 100 °C - 194 GPa
  • Testing temperature: 200 °C - 186 GPa
  • Testing temperature: 300 °C - 179 GPa
  • Testing temperature: 400 °C - 172 GPa
  • Testing temperature: 500 °C - 165 GPa

Mechanical properties od 1.4570 wires (+2D):

  • Diameter D: 0.05-0.10 mm - Rm: < 1100 MPa
  • Diameter D: 0.1-0.2 mm - Rm: < 1050 MPa
  • Diameter D: 0.2-0.5 mm - Rm: < 1000 MPa
  • Diameter D: 0.5-1.0 mm - Rm: < 950 MPa
  • Diameter D: 1-3 mm - Rm: < 900 MPa
  • Diameter D: 3-5 mm - Rm: < 850 MPa
  • Diameter D: > 5 mm - Rm: < 800 MPa

1.4570 mechanical properties in +1C, +1E, +1D, +1X, +1G, +2D condition:

  • Re: 220-250 MPa
  • Rm: 520-720 MPa
  • A: > 40 %
  • KV. 20°C: > 100 J
  • HBW: < 230

Mechanical properties of bright bars +2H, +2B, +2G, +2P:

  • Diameter D: < 16 mm
    • Re: > 400 MPa
    • Rm: 600-950 MPa
    • A: > 15 %
  • Diameter D: 16-63 mm
    • Re: > 185 MPa
    • Rm: 500-910 MPa
    • A: > 20 %
  • Diameter D: > 63 mm
    • Re: > 185 MPa
    • Rm: 500-710 MPa
    • A: > 35 %

Mechanical properties of 1.4570 wires in cold work-hardened condition (+2H):

  • +C500- Rm: 500-700
  • +C600- Rm: 600-800
  • +C700- Rm: 700-900
  • +C800- Rm: 800-1000
  • +C900- Rm: 900-1100
  • +C1000- Rm: 1000-1250
  • +C1100- Rm: 1100-1350
  • +C1200- Rm: 1200-1450
  • +C1400- Rm: 1400-1700
  • +C1600- Rm: 1600-1900
  • +C1800- Rm: 1800-2100

Heat treatment and working

Recommended working and heat treatment parameters for 1.4570 alloy:

  • Forging: 1150-900 °C
  • Rolling: 1150-900 °C
  • Solutioning: 1000-1100 °C

We deliver this steel alloy as:

  • Rods
  • Wires

Substitutes, equivalents and other species designations

1.4570
Z8CNUF18-09
SUS303Cu
303Cu
S30330
X6CrNiCuS18-9-2
UGI 303UX
UGIMA 303UX
UGI 4570
UGIMA 4570

Need help? Contact us!

Call or send a message, and our representative
will contact you within 24 hours!

We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie preferences
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.