Drawn wire from quality steel

Steel wires are made by cold drawing (sometimes hot) from wire rods with slightly larger diameter. They are characterized by high accuracy and surface smoothness, narrow dimensional tolerances, and high strength partly obtained after the process of drawing, apart heat treatment.

The company's offer includes thin wires, very thin wires, super thin wires, medium and thick. Considering the chemical composition, wires from martensitic steels, wires made of austenitic steels and wires of ferritic steel are supplied.

Wires are supplied in coils, spools, and straight sections with specified lengths and straightness. Considering the condition of delivery, the wires are soft, semi-hard and hard. In our offer we include:

Low-alloy carbon structural wires:

Carbon grades
C4C - 1.0303C8C - 1.0213C10C - 1.0214C15C - 1.0234
C20C - 1.0411C4D - 1.0300C7D - 1.0313C9D - 1.0304
C10D - 1.0310C12D - 1.0311C15D - 1.0413C48D - 1.0517
C50D - 1.0586C58D - 1.0609C60D - 1.0610C66D - 1.0612
C68D - 1.0613C70D - 1.0615C72D - 1.0617C76D - 1.0614
C78D - 1.0620C80D - 1.0622C82D - 1.0626C86D - 1.0616
C88D - 1.0628C92D - 1.0618C2D1 - 1.1185C3D1 - 1.1187
C4D1 - 1.1188C3D2 - 1.1110C5D2 - 1.1111C8D2 - 1.1113
C10D2 - 1.1114C12D2 - 1.1124C15D2 - 1.1126C18D2 - 1.1129
C2D1 - 1.1185C3D1 - 1.1187C4D1 - 1.1185C3D2 - 1.1110
C5D2 - 1.1111C8D2 - 1.1113C10D2 - 1.1113C12D2 - 1.1124
C15D2 - 1.1126C46D2 - 1.1162C48D2 - 1.1164C58D2 - 1.1212
C60D2 - 1.1226C62D2 - 1.1222C66D2 - 1.1236C70D2 - 1.1251
C72D2 - 1.1242C78D2 - 1.1252C82D2 - 1.1262C86D2 - 1.1265
C88D2 - 1.1272C92D2 - 1.1282C15E2C - 1.1132C17E2C - 1.1147
C20E2C - 1.1152C35EC - 1.117211SMn30 - 1.071511SMnPb30 - 1.0718

Structural alloy wires:

Wires for hardening and carburizing
17Cr3 - 1.701634Cr4 - 1.703337Cr4 - 1.703441Cr4 - 1.7035
18CrNi8 - 1.592025CrMo4 - 1.721834CrMo4 - 1.722042CrMo4 - 1.7225
34CrNiMo6 - 1.6582100Cr6 - 1.3505100CrMn6 - 1.352017B2 - 1.5502
18B2 - 1.550328B2 - 1.551033B2 - 1.551438B2 - 1.5515
20MnB4 - 1.552532CrB4 - 1.707636CrB4 - 1.707742CrMoS4 - 1.7227
23B2 - 1.550818MnB4 - 1.552123MnB4 - 1.553516MnCr5 - 1.7131

Spring and tool steel wires:

Spring and tool grades
51CrV4 - 1.815958CrV4 - 1.816159CrV4 - 1.224261CrSiV5 - 1.2243
73MoV5-2 - 1.238155Cr3 - 1.7176102Cr6 - 1.2067115CrV3 - 1.2210
N8E - C80W1 - 1.1525N10E - C105W1 - 1.154538Si7 - 1.502390MnCrV8 - 1.2842
120WV4 - 1.2516FDSiCrFDSiCrVTDSiCr
TDSiCrVVDSiCrVDSiCrVFDC
100Cr6 - 1.350580WV2 - 1.2517105WCr6 - 1.241931CrV3 - 1.2208
45SiCrV6 - 1.224945CrMoV7 - 1.232873MoV5-2 - 1.238190MnV8 - 1.2842

Druty żaroodporne i żarowytrzymałe:

Heat and creep resistant wires
X10CrAlSi7 - 1.4713X10CrAl14-4 - 1.4725X10CrAlSi18 - X10CrAl18 - 1.4742
X8CrAl25-5 - 1.4765X8CrAl20-5 - 1.4767X15CrNiSi25-21 - 1.4841
X15CrNiSi20-12 - 1.4828X8CrNi25-21 - 1.4845X6NiCrTiMoVB25-15-2 - 1.4980
X16NiCr30-20 - 1.4860X12NiCrSi35-16 - 1.4864X15CrNiSi25-4 - 1.4821
X12CrNi23-13 - 1.4833X22CrMoV12-1 - 1.492321CrMoV5-7 - 1.7709

Stainless and acid-resistant wires - high-alloyed:

Austenitic, ferritic, martensitic, and duplex steel wires
1.4301 - X5CrNi18-101.4303 - X4CrNi18-12
1.4305 - X8CrNiS18-91.4460 - X3CrNiMoN27-5-2
1.4306 - X2CrNi19-111.4307 - X2CrNi18-9
1.4310 - X10CrNi18-81.4401 - X5CrNiMo17-12-2
1.4404 - X2CrNiMo17-12-21.4435 - X2CrNiMo18-14-3
1.4436 - X3CrNiMo17-13-31.4438 - X2CrNiMo18-15-4
1.4539 - X1NiCrMoCu25-20-51.4429 - X2CrNiMoN17-13-3
1.4541 - X6CrNiTi18-101.4878 - X8CrNiTi18-10
1.4568 - X7CrNiAl17-71.4571 - X6CrNiMoTi17-12-2
1.4578 - X3CrNiCuMo17-11-3-21.4597 - X8CrMnCuNB17-8-3
1.4003 - X2CrNi121.4016 - X6Cr17
1.4113 - X6CrMo17-11.4112 - X90CrMoV18
1.4125 - X105CrMo171.4509 - X2CrTiNb18
1.4511 - X3CrNb171.4512 - X2CrTi12
1.4520 - X2CrTi171.4006 - X12Cr13
1.4021 - X20Cr131.4028 - X30Cr13
1.4034 - X46Cr131.4057 - X17CrNi16-2
1.4104 - X14CrMoS171.4122 - X39CrMo17-1
1.4362 - X2CrNiN23-41.4462 - X2CrNiMoN22-5-3

Kinds, grades and destination of wires

We offer wires:

 

  • corrosion-resistant, acid-resistant, and stainless, high alloyed
  • spring wires from alloy steel and carbon unalloyed steel
  • for thermal improvement and carburization
  • heat-resistant and chromium heat-resistant, chromium-nickel
  • made of precipitation strengthened, acid resistant steels
  • steel for heating and resistance elements
  • for swelling and cold extrusion
  • bearing steel and high speed HSS steel wires for drills
  • Duplex type made of high-alloy steel
  • from boiler steel for operation at elevated temperatures
  • nickel alloy and chromium alloy
  • titanium and titanium alloys
  • non-ferrous metals i.e. copper wires, brass wires, bronze wires
  • made of steel with special physical properties
  • brass, copper and other non-ferrous metals
  • tool steel, alloy steel and carbon steel
  • of alloys and special steels

 

Group of alloy steel available in wires:

  • CrSi, CrMn, CrMnSi, CrV, CrVSi, CrMo, CrMoV, CrW, CrWV
  • CrSiMo, CrSiMnMo, CrSiMoV, CrSiMnMoV, CrSiV, CrMnV, CrSiMnV, CrMoW, CrMoWV, CrSiTi, CrMnTi, CrSiMnTi
  • CrB, CrMnB, CrMnMoV, NiSi, NiMn, NiCu, NiMo, NiMoMn, NiMoCu, NiMoV, NiMnV
  • MnSiCu, MnSi, MnCr, MnCu, MnV, SiV, MnSiV, MnTi, SiTi, CrNiV, CrNiW, CrNiVW, CrNiMo

 

Surfaces and wire cross-sections
Round wires, cold-rolled, straight and in coilsFi 0,010 – fi 36mm tolerance H9,H10,H11

Szpule:

DIN 100

DIN 125

DIN 160

DIN 200

DIN 250

Hot drawn, dry drawn and wet drawn wires
Round, cold drawn straight wires, on rollers, spools or in coils
Round wires, ground, straight, on rollers, spools or in coils
Flat and square wires, drawn, on coils4 x 4 - 10 x 10mm tol. H11
Hexagonal and octagonal drawn wires on coils4 - 10mm tol. H11
Wires with cross section of regular and non-regular polygons

With regard to applications, we distinguish wires:

  • for springs for different purposes
  • for special screws, strings, staples, sheet metal screws, and rivets
  • for conveyor belts
  • for textile and construction industries
  • on braided and harp screens, string screens, woven mesh
  • for springs for automotive industry
  • for spirals and heating elements, for electric heaters
  • for needles, braids and brushes
  • for the production of fuel and air filters, for filter and catalytic sieves
  • for implants, prosthetics and jewelery
  • for the ropes for the mining and automotive industries
  • for sieves and heat-resistant mesh
  • for sorting and protective sieves for the mining industry
  • for vibration compensators

The products described above are determined by:

- Polish norms - PN-H-92603, PN-H-92604, PN-H-92611, PN-H-92612, PN-H-92600, PN-H-92601, PN-H-93003, PN-H-93222, PN-H-93223, PN-H-92610, PN-H-92336

 

- Euronorms - PN-EN 10263-1, PN-EN 10263-2, PN-EN 10263-3, PN-EN 10263-4, PN-EN 10263-5, PN-EN 10264-4, PN-EN 10270-1, PN-EN 10270-2, PN-EN 10270-3, PN-EN 10278, PN-EN 10277, EN ISO 16120, PN-EN 10016-2, PN-EN 10130, PN-EN 10016-4