DIN / EN ISO 1127 and ASME B36.10 / B36.19 Pipe Dimensions Table

The table compares the dimensions of steel pipes according to two different designation systems: DIN / EN ISO 1127 – the European system – and ASME B36.10 / B36.19 – the American system.

It can be used to find the American equivalent of the European DN designation. For example, DN 25 corresponds to a 1-inch pipe.

The table also provides the actual dimensions and weights of pipes manufactured in each series. For example, a DN 25 pipe in Series 3 has an outside diameter of 33.7 mm, a wall thickness of 2.6 mm, and a weight of 2.02 kg/m. Its closest American equivalent is a 1-inch schedule 10 pipe.

DN – diameter nominal, nominal diameter. This is NOT an exact diameter but an approximate designation.

OD – outside diameter, expressed in mm. The actual dimension specified by the relevant standards.

ASME NPS – nominal pipe size, the nominal pipe size according to ASME, expressed in inches. This is an approximate designation.

DIN Series 1–5 – a DIN production series describing wall thickness. Series 4 does NOT mean that the wall thickness is 4 mm. It is an approximate designation: generally, the higher the series number, the thicker the wall.

ASME Schedule 5S, 20, 160, XXS, etc. – an ASME designation describing wall thickness. Schedule 20 does NOT mean that the wall thickness is 20 mm or 2 inches. It is simply a designation used when ordering pipes. Generally, the higher the schedule number, the thicker the wall.

The weights given in the table apply to stainless steel pipes.

DIN ASME Pipe wall thickness [mm]
and weight [kg/m]
for DIN production series 1 to 5 and ASME production schedules from 5s to XXS

DN
 
OD
[mm]
NPS
[cal]
OD
[mm]
DIN
serie 1
ASME
schedule
5s
ASME
schedule
5
ASME 
schedule
10s
ASME 
schedule
10
DIN
serie 2
DIN
serie 3
ASME
schedule
STD 40s
DIN
serie 4
ASME
schedule
XS 80s
DIN
serie 5
ASME
schedule
20
ASME
schedule
30
ASME
schedule
40
ASME
schedule
60
ASME
schedule
80
ASME
schedule
100
ASME
schedule
120
ASME
schedule
140
ASME
schedule
160
ASME
schedule
XXS
6 10.2 1/8 10.29       1.24
0.28
1.24
0.28
    1.73
0.37
  2.41
0.48
    1.45
0.32
1.73
0.37
  2.41
0.48
         
8 13.5 ¼ 13.72       1.65
0.5
1.65
0.5
    2.21
0.64
  3.02
0.81
    1.85
0.55
2.21
0.64
  3.02
0.81
         
10 17.2 3/8 17.15       1.65
0.64
1.65
0.64
    2.31
0.86
  3.20
1.12
    2.11
0.79
2.31
0.86
  3.20
1.12
         
15 21.3 ½ 21.34 1.6
0.79
1.65
0.81
1.65
0.81
2.11
1.02
2.11
1.02
  2.0
0.97
2.77
1.29
3.2
1.45
3.73
1.64
4.0
1.73
  2.41
1.14
2.77
1.29
  3.73
1.64
      4.78
1.98
7.47
2.59
20 26.9 ¾ 26.67 1.6
1.01
1.65
1.03
1.65
1.03
2.11
1.3
2.11
1.3
  2.3
1.42
2.87
1.71
3.2
1.90
3.91
2.23
4.0
2.29
  2.41
1.46
2.87
1.71
  3.91
2.23
      5.56
2.94
7.82
3.69
25 33.7 1 33.4 2
1.59
1.65
1.31
1.65
1.31
2.77
2.12
2.77
2.12
  2.6
2.02
3.38
2.54
3.2
2.44
4.55
3.29
4.0
2.97
  2.90
2.21
3.38
2.54
  4.55
3.29
      6.35
4.30
9.09
5.53
32 42.4 1 ¼ 42.16 2
2.02
1.65
1.67
1.65
1.67
2.77
2.73
2.77
2.73
  2.6
2.59
3.56
3.44
3.6
3.50
4.85
4.53
4.0
3.85
  2.97
2.91
3.56
3.44
  4.85
4.53
      6.35
5.69
9.70
7.88
40 48.3 1 ½ 48.26 2
2.32
1.65
1.93
1.65
1.93
2.77
3.16
2.77
3.16
  2.6
2.98
3.68
4.11
4.0
4.44
5.08
5.49
5.0
5.42
  3.18
2.59
3.68
4.11
  5.08
5.49
      7.14
7.35
10.15
9.69
50 60.3 2 60.33 2
2.92
1.65
2.42
1.65
2.42
2.77
3.9
2.77
3.9
  2.9
4.17
3.91
5.52
4.5
6.29
5.54
7.60
5.6
7.67
  3.18
4.55
3.91
5.52
  5.54
7.60
      8.74
11.29
11.07
13.65
65 76.1 2 ½ 73.03 2.3
4.25
2.11
3.75
2.11
3.75
3.05
5.34
3.05
5.34
  2.9
5.32
5.16
8.77
5.0
8.90
7.01
11.59
7.1
12.27
  4.78
8.17
5.16
8.77
  7.01
11.59
      9.53
15.19
14.02
20.71
80 88.9 3 88.9 2.3
4.99
2.11
4.59
2.11
4.59
3.05
6.56
3.05
6.56
  3.2
6.87
5.49
11.47
5.6
11.68
7.62
15.51
8.0
16.20
  4.78
10.07
5.46
11.47
  7.62
15.51
      11.13
21.67
15.24
28.11
  101.6 3 ½ 101.6   2.11
5.26
2.11
5.26
3.05
7.53
3.05
7.53
    5.74
13.78
  8.08
18.92
    4.78
11.59
5.74
13.78
  8.08
18.92
         
100 114.3 4 114.3 2.6
7.27
2.11
5.93
2.11
5.93
3.05
8.50
3.05
8.50
  3.6
9.98
6.02
16.32
6.3
17.04
8.56
22.66
8.8
23.25
  4.78
13.11
6.03
16.32
  8.56
22.66
  11.13
28.75
  13.49
34.05
17.12
41.66
125 139.7 5 141.3 2.6
8.93
2.77
9.61
2.77
9.61
3.40
11.74
3.40
11.74
  4.0
13.59
6.55
22.10
6.3
21.04
9.53
31.44
10.0
32.47
    6.55
22.10
  9.53
31.44
  12.70
48.89
  15.88
49.87
19.05
58.31
150 168.3 6 168.28 2.6
10.79
2.77
11.48
2.77
11.48
3.40
14.04
3.40
14.04
4.0
16.46
4.5
18.46
7.11
28.69
7.1
28.66
10.97
43.21
11.0
43.32
    7.11
28.69
  10.97
43.21
  14.27
55.03
  18.26
68.59
21.95
80.42
200 219.1 8 219.08 2.9
15.7
2.77
15.0
2.77
15.0
3.76
20.27
3.76
20.27
4.5
24.18
6.3
33.57
8.18
43.20
8.0
42.29
12.70
65.63
12.5
64.66
6.35
33.82
7.04
33.38
8.18
43.20
10.31
53.89
12.70
65.63
15.09
77.07
18.26
91.95
20.62
102.46
23.01
112.96
22.23
109.57
250 273 10 273.05 2.9
19.61
3.40
22.96
3.40
22.96
4.19
28.21
4.19
28.21
5.0
33.55
6.3
42.07
9.27
61.23
8.8
58.21
12.70
82.79
14.2
92.02
6.35
42.40
7.80
51.80
9.27
61.23
12.70
82.79
15.09
97.47
18.26
116.49
21.44
135.07
25.40
157.50
28.58
174.94
25.40
157.50
300 323.9 12 323.85 2.9
23.31
3.96
31.72
3.96
31.72
4.57
36.53
4.57
36.53
5.6
44.63
7.1
56.32
9.53
75.00
10.0
78.60
12.70
98.94
16.0
123.35
6.35
50.48
8.38
66.19
10.31
80.94
14.27
110.61
17.48
134.09
21.44
162.34
25.40
189.81
28.58
211.30
33.32
242.38
25.40
189.81
350 355.6 14 355.6 3.2
28.24
3.96
34.87
3.96
34.87
4.78
41.99
6.35
55.53
5.6
49.08
8.0
69.63
9.53
82.58
11.0
94.91
12.70
109.04
17.5
148.15
7.92
68.95
9.53
82.58
11.13
96.00
15.09
128.66
19.05
160.53
23.83
197.96
27.79
228.10
31.75
257.46
35.71
286.02
 
400 406.4 16 406.4 3.2
32.31
4.19
42.2
4.19
42.2
4.78
48.07
6.35
63.61
6.3
63.11
8.8
87.61
9.53
94.70
12.5
123.28
12.70
125.19
20.0
193.50
7.92
79.02
9.53
94.70
12.70
125.19
16.66
162.58
21.44
206.66
26.19
249.33
30.96
291.04
36.53
338.30
40.49
370.96
 
450 457.2 18 457.2 4
45.39
4.19
47.53
4.19
47.53
4.78
54.15
6.35
71.68
6.3
71.13
10.0
111.97
9.53
106.82
14.2
157.51
12.70
141.35
22.2
241.80
7.92
89.09
11.13
124.31
14.27
158.26
19.05
208.99
23.83
285.58
29.36
314.52
34.93
369.32
39.67
414.72
45.24
466.64
 
500 508 20 508 4
50.48
4.78
60.23
4.78
60.23
5.54
69.70
6.35
79.76
6.3
79.14
11.0
136.89
9.53
118.94
16.0
197.10
12.7
157.50
25.0
302.34
9.53
118.94
12.70
157.50
15.09
186.24
20.625
251.63
26.19
315.95
32.54
387.38
38.10
448.27
44.45
515.91
50.01
573.48
 
  558.8 22 558.8   4.78
66.31
4.78
66.31
5.54
76.74
6.35
87.84
    9.53
131.07
  12.70
173.65
  9.53
131.07
12.70
173.65
  22.23
298.66
28.58
379.43
34.93
458.17
41.28
534.90
47.63
609.61
53.98
682.30
 
600 609.6 24 609.6 5
75.69
5.54
83.79
5.54
83.79
6.35
95.91
6.35
95.91
6.3
95.17
12.5
186.88
9.53
143.19
17.5
259.44
12.70
189.81
30.0
435.37
9.53
143.19
14.27
212.71
17.48
259.15
24.61
360.47
30.96
448.56
38.89
555.73
46.02
649.40
52.37
730.68
59.54
820.02
 
    26 660.4               9.53
155.31
  12.70
205.96
  12.70
205.95
                 
700 711 28 711.2 5
88.39
        7.1
125.13
12.5
218.62
9.53
167.43
  12.70
222.12
  12.70
222.12
15.88
276.47
               
    30 762   6.35
120.14
6.35
120.14
7.92
149.54
7.92
149.54
    9.53
179.55
  12.70
238.27
  12.70
238.27
15.88
296.67
               
800 813 32 812.8 5.6
113.21
        8.0
161.25
12.5
250.54
9.53
191.67
  12.70
254.42
  12.70
254.42
15.88
316.86
17.48
348.09
             
    34 863.6               9.53
203.80
  12.70
270.58
  12.70
270.58
15.88
337.06
17.48
370.32
             
900 914 36 914.4 6.3
143.18
        10.0
226.35
12.5
282.15
9.53
215.92
  12.70
286.73
  12.70
286.73
15.88
357.26
19.05
427.07
             

 

Quick Reference – DN to Inch Conversion

  • DN 6 corresponds to 1/8 inch
  • DN 8 corresponds to 1/4 inch
  • DN 10 corresponds to 3/8 inch
  • DN 15 corresponds to 1/2 inch
  • DN 20 corresponds to 3/4 inch
  • DN 25 corresponds to 1 inch
  • DN 32 corresponds to 1 1/4 inches
  • DN 40 corresponds to 1 1/2 inches
  • DN 50 corresponds to 2 inches
  • DN 65 corresponds to 2 1/2 inches
  • DN 80 corresponds to 3 inches
  • DN 100 corresponds to 4 inches
  • DN 125 corresponds to 5 inches
  • DN 150 corresponds to 6 inches
  • DN 200 corresponds to 8 inches
  • DN 400 corresponds to 16 inches
  • And so on – as a rough rule of thumb, every additional 25 DN corresponds to approximately 1 inch.

Post author

Piotr Sompoliński

CSO Virgamet

Need help? Contact us!

Call or send a message, and our representative
will contact you within 24 hours!

We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie preferences
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.