Cold work tool steel 73MoV5-2, 1.2381

Standard Steel Grade
Chemical composition %
C: Mn: Si: P: S: Mo: V:
DIN 73MoV5-2 - 1.2381
0.70 - 0.77 0.4 - 0.6 1.0 - 1.3 <0.025 <0.025 0.45 - 0.65 0.15 - 0.25

 

Specification and applications of 73MoV5-2, 1.2381 steel grade

High-carbon tool steel with added Vanadium and Molybdenum, characterized by high strength, torsional and fatigue resistance, for the production of basic high hardness tools. Similar to the N7E, N8E tool grades in the enriched version with alloying additives. Main applications are guillotines, punches, screwdrivers, threading dies, knives and blades. The hardened steel reaches a hardness of 64 HRC.

 


Heat treatment

  • Annealing at a temperature of 700-750C with cooling in furnace
  • Relief annealing at a temperature of 650-680C with cooling in furnace
  • Hardening at a temperature of 840-860C with cooling in oil
  • Tempering at temperature:
    • 100C = 64 HRC
    • 200C = 59-60 HRC
    • 300C = 55-56 HRC
    • 400C = 52 HRC
    • 500C = 48 HRC
    • 600C = 45 HRC

 


In the above mentioned grades the company delivers:

 


Other designations of the grade:

73 MoV 5-2, 1.2381, AISI S2, UNS T41902


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.