31CrV3, 31CrV2, 1.2208 - Tool steel for cold working according to DIN 17350.

Standard Steel Grade
Chemical composition %
C: Mn: Si: P: S: Cr: V: Cu:
DIN 31CrV3 - 31CrV2 - 1.2208
0.28 - 0.35 0.40 - 0.60 0.25 - 0.40 <0.030 <0.030 0.40 - 0.70 0.07 - 0.12 -
STAS 31VCr5
0.28 - 0.35 0.40 - 0.60 0.25 - 0.40 <0.030 <0.030 0.40 - 0.70 0.07 - 0.12 <0.3
NF 31CV3
0.28 - 0.35 0.40 - 0.60 0.25 - 0.40 <0.030 <0.030 0.40 - 0.70 0.07 - 0.12 -
GOST 3ChF - 3ХФ
0.28 - 0.35 0.40 - 0.60 0.25 - 0.40 <0.030 <0.030 0.40 - 0.70 0.07 - 0.12 -

 


31CrV2, 1.2208 - specification and application

Cold working tool steel for basic everyday mechanical tools such as screwdrivers, wrenches, screwdrivers, sockets. Water-hardening steel.


Mechanical properties:

  • Annealed condition +A: <220 HB
  • Hardness after hardening: 52-54 HRC
  • Hardness after tempering at temperature:
    • 100C = 52 HRC
    • 200C = 50 HRC
    • 300C = 47 HRC
    • 400C = 43 HRC
    • 500C = 44 HRC

Heat treatment

  • Softening annealing at 700 +/-20C with air cooling
  • Hardening at a temperature of 845 +/-15C with water cooling
  • Stress relief annealing at a temperature of 665 - 15C

In the above mentioned grades the company delivers:


Other designations of the grade:

31VCr5, 31CV3, 3ChF, 3ХФ


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.