26NiCrMo14-5, 1.6953, 26NiCrMo14-6, 1.6958 - structural case-hardening steel for carburizing according to DIN 17210.

Standard Steel Grade
Chemical Composition %
C: Mn: Si: P: S: Cr: Mo: Ni: V:
DIN 26NiCrMo14-6 - 1.6958
0.28 - 0.38 0.15 - 0.40 <0.40 <0.035 <0.035 1.0 - 1.7 0.3 - 0.6 2.9 - 3.8 0.08 - 0.25
EN 26NiCrMo14-5 - 1.6953
0.22 - 0.30 0.20 - 0.50 <0.40 <0.035 <0.035 1.0 - 1.7 0.3 - 0.6 3.2 - 4.0 <0.15
SEW 33NiCrMo14-6 - 1.6956
0.28 - 0.36 0.20 - 0.50 <0.40 <0.035 <0.035 1.0 - 1.7 0.3 - 0.6 3.2 - 4.0 <0.15
NF 25NCD15
0.20 - 0.30 0.20 - 0.50 0.10 - 0.35 <0.030 <0.025 1.1 - 1.4 0.35 - 0.60 3.7 - 4.2 -

 


26NiCrMo14-6, 1.6958, 26NiCrMo14-5, 1.6953 - specifications and applications

Alloy carburizing steel for special, most heavily loaded machine parts requiring high surface hardness and high core strength, including ductility.

 


In the above-mentioned grade the company offers:


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.