C: Si: Mn: P: S: Cr: Mo: Ni: Ti: Cu: N: W: V:
GOST 25ChGT - 25HGT
0.22-0.29 0.17-0.37 0.8-1.1 <0.035 <0.035 1.0-1.3 <0.15 <0.3 0.03-0.09 <0.3 <0.008 <0.05 <0.2
GOST 30ChGT - 30HGT
0.24-0.32 0.17-0.37 0.8-1.1 <0.035 <0.035 1.0-1.3 <0.15 <0.3 0.03-0.09 <0.3 <0.008 <0.05 <0.2
DIN 30MnCrTi4 / 1.8401
0.25-0.35 0.15-0.35 0.9-1.2 <0.025 <0.025 0.8-1.0 0.15-0.30 - - - - - -

25HGT, 1.8401, 30MnCrTi4, 30HGT – description

Case-carburizing steel 25HGT has greater amount of carbon than similar alloy 18HGT. The grade shows higher hardness after heat treatment than 18HGT. The rest of the alloy additions are similar.


Applications

This alloy is widely used for:

  • Gears
  • Transmission shafts

Physical and mechanical properties

A very ductile and shock-resistant steel. Hard top layer after carburizing.

  • Yield strength: >980 MPa
  • Tensile strength: >1270 MPa
  • Elongation: 10%
  • Impact Value KCU, 20°C: 69 J/sm2
  • Hardness after tempering: <217HB

We can deliver:


Replacements, equivalents and other designations:

25ChGT, 25ChGT-Sh, 25ChGTA, 25ХГТ, 25ChGTA-Sh, 30ChGT, 30ChGT-Sh, 30CrMnTi, 1.8401, 30MnCrTi4, 30ХГТ


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.