Tool steel for cold working 1.2999, X45MoCrV5-3-1.

Standard Steel Grade
Chemical composition %
C: Mn: Si: Cr: Mo: V:
DIN X45CrMoV5-3-1 - 1.2999
0.45 0.30 0.30 3.00 5.00 1.00

 

X45MoCrV5-3-1, 1.2999 - specification and application

Hot working tool steel with the highest resistance to loads, impacts and shocks, high resistance to temperature fluctuations and tempering. It is also characterized by high thermal conductivity, resistance to critical temperatures and fatigue. Material 1.2999 is the right choice for the production of heavy-duty dies, forging tools, casting moulds for demanding metals and other applications where the highest purity of the material is required.


Mechanical properties of 1.2999

  • Hardness in annealed condition <230HB
  • Hardness after hardening: 56-57HRC
  • Thermal conductivity: 31.4 W*m-1*K-1
  • Hardness after hardening and tempering at temperature:
    • 300C = 54HRC
    • 400C = 55HRC
    • 500C = 56HRC
    • 550C = 57HRC
    • 600C = 53HRC

Heat treatment of X45CrMoV5-3-1 - processes and temperatures:

  • Softening annealing at a temperature of 750-800C
  • Hardening at a temperature of 1070 - 1100C with cooling in oil
  • Tempering at temperature 500-550C

In the above mentioned grade we deliver:


We use cookies
In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy. You can specify the detailed configuration by clicking the button below "Settings".
Cookie settings
We use cookies

In order to properly operate the Website and for statistical purposes, and if you consent, also to personalize advertising, remarketing and retargeting. If you want to learn more, read on privacy and cookies policy.

More information

If you have any questions about our cookie policy, please ask contact.